REINFORCED ARTICLES AND METHODS OF MAKING THE SAME
    11.
    发明申请
    REINFORCED ARTICLES AND METHODS OF MAKING THE SAME 有权
    强化制品及其制造方法

    公开(公告)号:US20140120308A1

    公开(公告)日:2014-05-01

    申请号:US13664123

    申请日:2012-10-30

    Abstract: An article comprising a substrate; a bond layer disposed on the substrate, the bond layer comprising one or more bonding segments and at least one reinforcing segment; at least one protective layer disposed on the bond layer; and at least one cooling hole extending through the substrate, the at least one reinforcing segment and the at least one protective layer, wherein the at least one reinforcing segment reduces cracking and/or delamination at the interface between the substrate and the bond layer, and methods of making the same.

    Abstract translation: 一种包含基材的制品; 设置在所述基板上的接合层,所述接合层包括一个或多个接合段和至少一个加强段; 设置在所述接合层上的至少一个保护层; 以及延伸穿过基底,至少一个加强段和至少一个保护层的至少一个冷却孔,其中所述至少一个加强段减少在基底和接合层之间的界面处的裂纹和/或分层,以及 制作相同的方法

    Cast nickel-base superalloy including iron

    公开(公告)号:US11001913B2

    公开(公告)日:2021-05-11

    申请号:US16283269

    申请日:2019-02-22

    Abstract: A cast nickel-base superalloy that includes iron added substitutionally for nickel. The cast nickel-base superalloy comprises, in weight percent about 1-6% iron, about 7.5-19.1% cobalt, about 7-22.5% chromium, about 1.2-6.2% aluminum, optionally up to about 5% titanium, optionally up to about 6.5% tantalum, optionally up to about 1% Nb, about 2-6% W, optionally up to about 3% Re, optionally up to about 4% Mo, about 0.05-0.18% C, optionally up to about 0.15% Hf, about 0.004-0.015 B, optionally up to about 0.1% Zr, and the balance Ni and incidental impurities. The superalloy is characterized by a γ′ solvus temperature that is within 5% of the γ′ solvus temperature of the superalloy that does not include 1-6% Fe and a mole fraction of γ′ that is within 15% of the mole fraction of the superalloy that does not include 1-6% Fe.

    ARTICLE AND METHOD FOR FORMING AN ARTICLE
    14.
    发明申请
    ARTICLE AND METHOD FOR FORMING AN ARTICLE 审中-公开
    文章和形成文章的方法

    公开(公告)号:US20160326613A1

    公开(公告)日:2016-11-10

    申请号:US14706151

    申请日:2015-05-07

    Abstract: An article and a method for forming the article are disclosed. The article comprising a composition, wherein the composition comprises, by weight percent, about 20.0% to about 22.0% chromium (Cr), about 18.0% to about 20.0% cobalt (Co), about 1.0% to about 2.0% tungsten (W), about 3.0% to about 6.0% niobium (Nb), about 0.5% to about 1.5% titanium (Ti), about 2.0% to about 3.0% aluminum (Al), about 0.5% to about 1.5% molybdenum (Mo), about 0.03% to about 0.18% carbon (C), up to about 0.15% tantalum (Ta), up to about 0.20% hafnium (Hf), up to about 0.20% iron (Fe),balance nickel (Ni) and incidental impurities. The amount of Al is present according to the following formula: Al≦−(0.5*Ti)+3.75 The composition is weldable, has a microstructure comprising between about 35 vol % and 45 vol % gamma prime (γ′) and is substantially devoid of Eta and reduced content of TCP phases at elevated working temperatures. A method of making an article and a method of operating a gas turbine are also disclosed.

    Abstract translation: 组合物是可焊接的,具有包含约35vol%至45vol%的γ'(γ')的微结构,并且在升高的工作温度下基本上不含Eta并且降低了TCP相的含量。 还公开了制造物品的方法和操作燃气轮机的方法。

    MATERIALS FOR DIRECT METAL LASER MELTING
    15.
    发明申请
    MATERIALS FOR DIRECT METAL LASER MELTING 审中-公开
    直接金属激光熔炼材料

    公开(公告)号:US20160082511A1

    公开(公告)日:2016-03-24

    申请号:US14491471

    申请日:2014-09-19

    Abstract: A nickel alloy for direct metal laser melting is disclosed. The alloy comprising includes a powder that contains about 1.6 to about 2.8 weight percent aluminum, about 2.2 to about 2.4 weight percent titanium, about 1.25 to about 2.05 weight percent niobium, about 22.2 to about 22.8 weight percent chromium, about 8.5 to about 19.5 weight percent cobalt, about 1.8 to about 2.2 weight percent tungsten, about 0.07 to about 0.1 weight percent carbon, about 0.002 to about 0.015 weight percent boron, and about 40 to about 70 weight percent nickel. Related processes and articles are also disclosed.

    Abstract translation: 公开了一种用于直接金属激光熔化的镍合金。 包括的合金包括含有约1.6至约2.8重量%的铝,约2.2至约2.4重量%的钛,约1.25至约2.05重量%的铌,约22.2至约22.8重量%的铬,约8.5至约19.5重量的粉末 约1.8至约2.2重量%的钨,约0.07至约0.1重量%的碳,约0.002至约0.015重量百分比的硼和约40至约70重量%的镍。 还公开了相关方法和制品。