METHOD FOR PRODUCING MODIFIED ANIMAL FIBER
    159.
    发明申请
    METHOD FOR PRODUCING MODIFIED ANIMAL FIBER 有权
    生产改性动物纤维的方法

    公开(公告)号:US20110191963A1

    公开(公告)日:2011-08-11

    申请号:US13063375

    申请日:2010-06-23

    IPC分类号: D06M11/34

    摘要: Disclosed is a method for producing a modified animal fiber, the method includes step 1 (31, 32) of pre-oxidizing a cystine bond (—S—S— bond) present in an epidermal cell of an animal fiber to bring the cystine bond into a low oxidation state, step 2 (33) of oxidizing with ozone the pre-oxidized —S—S— bond to bring the —S—S— bond into at least one high oxidation state selected from di-, tri-, and tetra-oxidation states, and step 3 (34) of reductively cleaving the —S—S— bond in a high oxidation state. The method imparts shrink resistance and pilling resistance to an animal fiber. In the step 2 (33) ozone is microdispersed in an aqueous solution comprising an anionic surfactant having a C8-24 alkyl group, and the animal fiber is contacted with the ozone. Accordingly, the present invention provides a method for efficiently producing in a short period of time an animal fiber having excellent shrink resistance that barely undergoes felting when washed in an aqueous system in shrink proofing an animal fiber using ozone.

    摘要翻译: 公开了一种改性动物纤维的制造方法,其特征在于,包括步骤1(31,32),其对存在于动物纤维表皮细胞中的胱氨酸键(-S-S-键)进行预氧化以使胱氨酸键 进入低氧化状态,步骤2(33)用臭氧氧化预氧化的-S-S-键,使-S-S-键进入至少一个选自二,三和 以及在高氧化态下还原性裂解-S-S-键的步骤3(34)。 该方法赋予动物纤维的抗收缩性和起球抗性。 在步骤2(33)中,臭氧被微分散在包含具有C8-24烷基的阴离子表面活性剂的水溶液中,动物纤维与臭氧接触。 因此,本发明提供了一种用于在短时间内有效地生产在使用臭氧收缩动物纤维的水性体系中洗涤时几乎不发生熔融的抗收缩性优异的动物纤维。