Invention Application
- Patent Title: APPARATUS LINE FOR MANUFACTURING SEAMLESS STEEL PIPE AND TUBE AND METHOD OF MANUFACTURING DUPLEX SEAMLESS STAINLESS STEEL PIPE
-
Application No.: US15529842Application Date: 2015-10-07
-
Publication No.: US20170335422A1Publication Date: 2017-11-23
- Inventor: Shunsuke Sasaki , Tatsuro Katsumura , Hiroki Ushida , Yasushi Kato
- Applicant: JFE STEEL CORPORATION
- Applicant Address: JP Tokyo
- Assignee: JFE STEEL CORPORATION
- Current Assignee: JFE STEEL CORPORATION
- Current Assignee Address: JP Tokyo
- Priority: JP2014-239449 20141127
- International Application: PCT/JP2015/005095 WO 20151007
- Main IPC: C21D9/08
- IPC: C21D9/08 ; B21B3/02 ; C22C38/48 ; C22C38/46 ; C22C38/44 ; C22C38/42 ; C22C38/06 ; C22C38/04 ; C22C38/02 ; C22C38/00 ; C22C30/00 ; C22C38/50 ; B21B17/08 ; B21B19/04 ; C21D8/10 ; C21D6/00 ; B21B45/02 ; B21B45/00 ; C22C38/54

Abstract:
An apparatus line for manufacturing seamless steel pipes and tubes includes: a heating apparatus for heating a steel raw material; a piercing apparatus for piercing the heated steel raw material thus forming a hollow material; and a rolling apparatus for applying working to the hollow material to form a seamless steel pipe having a predetermined shape. A cooling apparatus is arranged on an exit side of the rolling apparatus. A heated steel raw material is worked by the rolling apparatus after being pierced by the piercing apparatus, and thereafter, using a surface temperature of a hollow piece before being cooled by the cooling apparatus as a cooling start temperature, the hollow piece is cooled to a cooling stop temperature differing by 50° C. or more from the cooling start temperature and being equal to or above 600° C. at an average cooling speed of 1.0° C./s or more in terms of an outer surface temperature.