Optical laminate including reddening-resistant layer
摘要:
An optical laminate, including: a polarizing layer; and a porous layer formed on at least one side of the polarizing layer, wherein the polarizing layer includes zinc component, and wherein an absolute value of a change in an amount of color coordinate a* of CIE L*a*b* according to Equation 1 is 2 or less:

Δa*=a*a−a*i  [Equation 1]



wherein Δa* is the change in the amount of the color coordinate a*, a*a is a color coordinate a* of the optical laminate after maintaining the optical laminate at 105° C. for 250 hours under a state where both top and bottom surfaces of the optical laminate come in contact with glass substrates, and a*i is a color coordinate a* of the optical laminate before maintaining the optical laminate at 105° C. for 250 hours.
公开/授权文献