- 专利标题: Glass containers with improved strength and improved damage tolerance
-
申请号: US16653974申请日: 2019-10-15
-
公开(公告)号: US11951072B2公开(公告)日: 2024-04-09
- 发明人: Dana Craig Bookbinder , Theresa Chang , Paul Stephen Danielson , Steven Edward DeMartino , Andrei Gennadyevich Fadeev , Robert Michael Morena , Santona Pal , John Stephen Peanasky , Robert Anthony Schaut , Christopher Lee Timmons , Natesan Venkataraman , Ronald Luce Verkleeren
- 申请人: CORNING INCORPORATED
- 申请人地址: US NY Corning
- 专利权人: Corning Incorporated
- 当前专利权人: Corning Incorporated
- 当前专利权人地址: US NY Corning
- 代理机构: Dinsmore & Shohl LLP
- 分案原申请号: US15331120 2016.10.21
- 主分类号: A61J1/14
- IPC分类号: A61J1/14 ; A61J1/06 ; B32B17/06 ; B65D1/02 ; B65D1/40 ; B65D23/02 ; B65D23/08 ; B65D25/14 ; B65D25/34 ; B65D65/42 ; C03B23/04 ; C03C15/02 ; C03C17/00 ; C03C17/22 ; C03C17/30 ; C03C17/32 ; C03C17/34 ; C03C17/42 ; C03C21/00 ; C09D179/08
摘要:
A coated glass pharmaceutical package includes a glass body having a Type 1 chemical durability according to USP 660, at least a class A2 base resistance or better according to ISO 695, and at least a type HGB2 hydrolytic resistance or better according to ISO 719, the glass body having an interior surface and an exterior surface and a wall extending therebetween. A lubricous coating having a thickness of less than or equal to 90 nm may be positioned on at least a portion of the exterior surface of the glass body but not on any portion of the interior surface. The portion of the coated glass package with the lubricous coating comprises a coefficient of friction that is at least 20% less than an uncoated glass package and the coefficient of friction does not increase by more than 30% after undergoing a depyrogenation cycle including exposure to a temperature of 250° C. for a time period of 30 minutes. A horizontal compression strength of the coated glass package is at least 10% greater than an uncoated glass package and the horizontal compression strength is not reduced by more than 20% after undergoing the depyrogenation cycle including exposure to a temperature of 250° C. for a time period of 30 minutes and then being abraded. The lubricous coating comprises a polymer.
公开/授权文献