Abstract:
A polymer composition having satisfactory processing stability is provided which comprises a polymer; a bisphenol monoester represented by the Formula (1): wherein R1 represents hydrogen, alkyl or phenyl group; R2 and R3 each independently represents alkyl group; and R4 and R5 each independently represents hydrogen or methyl group; and a bisphenol diester represented by Formula (2) wherein R6 represents hydrogen, alkyl or phenyl group; R7 and R8each independently represents alkyl group; and R9 and R10 each independently represents hydrogen or methyl group in which amount of the compound of formula (2) is 0.001 to 5 parts by weight based on 100 parts by weight of the total amount of the compounds of formulae (1) and (2).
Abstract:
The invention relates to synergistic combinations of certain phenolic antioxidants in thermoplastic polymers, especially in polyolefin pipes and other thermoplastic molding materials which are in prolonged contact with water. The instant combinations lead to better resistance against oxidative degradation as measured in terms of oxidation induction times (OIT), color and other technically important parameters as known in the art.
Abstract:
There are described compositions comprising a) an emulsion crude rubber, synthetic latex or natural rubber latex subject to oxidative, thermal, dynamic and/or light-induced degradation, and b) as stabilizer at least one compound of formula I wherein R1 is C8-C20alkyl; and optionally c) as further stabilizer at least one compound of formula II wherein R2 is C8-C12alkyl, R3 is hydrogen, C1-C12alkyl, cyclohexyl, 1-methylcyclohexyl, benzyl, &agr;-methylbenzyl, &agr;,&agr;-dimethylbenzyl or —CH2—S—R2, R4 is C1-C12alkyl, benzyl, &agr;-methylbenzyl, 60 ,&agr;-dimethylbenzyl or —CH2—S—R2, and R5 is hydrogen or methyl.