Binder mixtures crosslinkable by radiation
    1.
    发明授权
    Binder mixtures crosslinkable by radiation 失效
    BINDER混合物通过辐射交联

    公开(公告)号:US5102702A

    公开(公告)日:1992-04-07

    申请号:US733424

    申请日:1991-07-22

    摘要: Binder mixtures crosslinkable by radiation comprising as component A a product obtained by reaction of an epoxy compound with more than one epoxide group per molecule with at least one carboxylic acid in a molar ratio of epoxide groups to carboxyl groups of 1:0.5-0.9 and subsequent reaction of the reaction product with at least one unsaturated isocyanatocarbamate esters and as component B a product obtained by reaction of an epoxy compound with more than one epoxide group per molecule with at least one olefinic unsaturated carboxylic acid in a molar ratio of epoxide groups to carboxyl groups of 1:>>1 and subsequent reaction of the reaction product with at least one polybasic carboxylic acid or anhydride(s) thereof, components A and B being present in a weight ratio of 3:1 to 1:3 useful for the product of superior photo-resists and protective lacquers.

    摘要翻译: 通过辐射可交联的粘合剂混合物,其包含通过环氧化合物与每个分子具有多于一个环氧基团的环氧化合物与至少一种环氧基团与羧基摩尔比为1:0.5-0.9的羧酸反应获得的产物,随后 反应产物与至少一种不饱和异氰酸酯基氨基甲酸酯反应,并且作为组分B,通过环氧化合物与每个分子具有多于一个环氧基的反应获得的产物与至少一种以环氧基团与羧基的摩尔比的烯属不饱和羧酸反应 基团1:>> 1,随后将反应产物与至少一种多元羧酸或其酸酐反应,组分A和B以3:1至1:3的重量比存在,可用于产物 优异的光刻胶和保护漆。

    One-component thermosetting coating composition
    4.
    发明授权
    One-component thermosetting coating composition 失效
    单组分热固性涂料组合物

    公开(公告)号:US6025438A

    公开(公告)日:2000-02-15

    申请号:US716250

    申请日:1997-01-15

    摘要: A one-component thermosetting coating composition containing of one or more chemically setting binders, at least one curing or crosslinking agent, and one or more toughening substances, the composition being semisolid and tackfree at temperatures

    摘要翻译: PCT No.PCT / EP95 / 00864 Sec。 371日期1997年1月15日 102(e)日期1997年1月15日PCT Filed Mar. 9,1995 PCT Pub。 公开号WO95 / 25147 日期1995年9月21日一种含有一种或多种化学固化粘合剂,至少一种固化或交联剂和一种或多种增韧物质的单组分热固性涂料组合物,该组合物在50℃温度下为半固体和无粘性, 其中所述化学固化粘合剂具有500至250,000之间的平均分子量(+ E,ovs M + EE w),熔点大于50℃,玻璃化转变温度高于20℃并固化 完全在80至250℃的温度下进行,并且在15秒内达到最终强度的至少10%,其中粘合剂具有作为反应性基团的环氧基或烯属不饱和基团,其中选择增韧物质 由具有末端羧基,环氧化物,氨基或烯属不饱和基团的丁二烯 - 丙烯腈共聚物组成的组或是高度支化的脂族烃环氧化物,其中在至少一种固化或 交联剂是通式M(SR)xBz的金属络合物,其中M =金属离子,L =配体,SR =酸根离子,B =路易斯碱,x = 1至8的数,以及 z = 7至8的数,并且其中如果需要,组合物可含有其它添加剂。