1.
公开(公告)号:US20240101472A1
公开(公告)日:2024-03-28
申请号:US18354757
申请日:2023-07-19
Applicant: Samsung Display Co., Ltd.
Inventor: WON-JONG BAEK , TAEHO AN
CPC classification number: C03C21/005 , C03C21/002 , H05K5/03
Abstract: Provided is a method of manufacturing a window, which includes preparing a first preliminary glass substrate including Li+ ions and Na+ ions, providing a first strengthening molten salt including Na+ ions onto the first preliminary glass substrate and forming a second preliminary glass substrate, providing a second strengthening molten salt including Rb+ ions onto the second preliminary glass substrate and forming a third preliminary glass substrate, and providing a third strengthening molten salt including K+ ions onto the third preliminary glass substrate and forming a strengthened glass substrate.
-
公开(公告)号:US20240343640A1
公开(公告)日:2024-10-17
申请号:US18406822
申请日:2024-01-08
Applicant: Samsung Display Co., Ltd.
Inventor: TAEHO AN , WON-JONG BAEK , MYUNGHUN BAEK , JEONG SEOK LEE
CPC classification number: C03C21/002 , H05K5/03
Abstract: A window includes a tempered glass substrate that includes a base layer and a compressive stress layer including a first region and a second region. The second region includes a first portion that includes a first point and is adjacent to the first region, a second portion that includes a second point and is adjacent to the base layer, and a third portion that includes a third point and that is disposed between the first portion and the second portion. A compressive stress at the first point is in a range of about 100 MPa to about 250 MPa, a compressive stress at the second point is in a range of about 50 MPa to about 150 MPa, and a compressive stress at the third point is in a range of about 70 MPa to about 200 MPa.
-
公开(公告)号:US20230312411A1
公开(公告)日:2023-10-05
申请号:US18098941
申请日:2023-01-19
Applicant: Samsung Display Co., Ltd.
Inventor: TAEHO AN , JEONG SEOK LEE , JUN HAK OH , SOOKKYUNG YOU , HYUN-IL CHO
IPC: C03C21/00
CPC classification number: C03C21/002 , C03C2203/52
Abstract: A method of manufacturing a window, includes: preparing a first preliminary glass substrate that does not contain Li+ ions and contains Na+ ions; providing a first strengthening molten salt to the first preliminary glass substrate to form a second preliminary glass substrate; providing heat to the second preliminary glass substrate at a temperature of about 400 to 500° C. for a period of about 3 to 7 hours to form a third preliminary glass substrate; and providing a second strengthening molten salt to the third preliminary glass substrate to form a window.
-
-