公开(公告)号:US10377859B2
公开(公告)日:2019-08-13
申请号:US15541497
申请日:2016-01-04
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Viswanathan Kalyanaraman , Nitin Vilas Tople
Abstract: Disclosed herein is a friable polyimide powder having a weight average molecular weight, as determined by gel permeation chromatography (GPC) using polystyrene standards, of less than or equal to 24,500 Daltons and a reactive aromatic amine end group concentration greater than or equal to 3 mole percent, wherein 90 weight percent of the powder particles are reducible to less than or equal to 75 micrometers by mechanical grinding. Also disclosed is a method of making the friable polyimide powder, a processed polyimide resulting from the friable polyimide powder and compositions comprising the processed polyimide.
-
公开(公告)号:US20200270398A1
公开(公告)日:2020-08-27
申请号:US16646663
申请日:2018-09-19
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Nitin Vilas Tople , Bernabe Quevedo Sanchez , Gregory L. Hemmer
IPC: C08G73/10
Abstract: A method of making a polyetherimide includes forming an intermediate polyetherimide with an anhydride-amine stoichiometry of −2 to −40 mol % and melt mixing the intermediate polyetherimide with a bis(ether anhydride) for greater than 3 minutes at a temperature 50 to 225° C. greater than the glass transition temperature of a final polyetherimide to produce the final polyetherimide.
-
公开(公告)号:US20180016395A1
公开(公告)日:2018-01-18
申请号:US15541497
申请日:2016-01-04
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Viswanathan Kalyanaraman , Nitin Vilas Tople
CPC classification number: C08G73/1053 , C08G73/1078 , C08J3/12 , C08J2379/08 , C08L33/14 , C08L63/00 , C08L79/08
Abstract: Disclosed herein is a friable polyimide powder having a weight average molecular weight, as determined by gel permeation chromatography (GPC) using polystyrene standards, of less than or equal to 24,500 Daltons and a reactive aromatic amine end group concentration greater than or equal to 3 mole percent, wherein 90 weight percent of the powder particles are reducible to less than or equal to 75 micrometers by mechanical grinding. Also disclosed is a method of making the friable polyimide powder, a processed polyimide resulting from the friable polyimide powder and compositions comprising the processed polyimide.
-
公开(公告)号:US20200231753A1
公开(公告)日:2020-07-23
申请号:US16647780
申请日:2018-09-19
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Nitin Vilas Tople , Viswanathan Kalyanaraman , Kelly Leung , Thomas Link Guggenheim
IPC: C08G73/10
Abstract: A method for modifying a polyimide includes reacting a first polyimide with an amine to produce a second polyimide having an anhydride-amine stoichiometry of −2 to −40 mol % and reacting the second polyimide with a monoanhydride, a bis(anhydride), a bis(ether anhydride) or a tetracarboxylic acid to produce a final polyimide having an anhydride-amine stoichiometry of −1 to 2 mol %.
-
公开(公告)号:US20200216615A1
公开(公告)日:2020-07-09
申请号:US16647793
申请日:2018-09-19
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Nitin Vilas Tople , Bernabe Quevedo Sanchez , Juan Justino Rodriguez Ordonez , Javier Nieves Remacha , Yusuf Sulub
IPC: C08G73/10
Abstract: A method of making a polyetherimide includes melt mixing a composition comprising an aromatic bis(ether anhydride) and a diamine to form a polyetherimide wherein melt mixing occurs at a temperature 50 to 225° C. greater than the glass transition temperature of the polyetherimide and after the composition attains a weight average molecular weight that is greater than or equal to 20% of the weight average molecular weight of the polyetherimide melt mixing occurs at a pressure less than atmospheric pressure.
-
公开(公告)号:US10793675B2
公开(公告)日:2020-10-06
申请号:US16302428
申请日:2017-05-23
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Thomas Link Guggenheim , Nitin Vilas Tople , Karthik Venkataraman
Abstract: A method of making a polyetherimide comprises: combining a bisphenol A dianhydride, p-phenylene diamine and a halogenated aromatic solvent to form a reactant solution; heating the reactant solution to a temperature of 205° C. to 330° C. at a pressure sufficient to prevent boiling to afford a reaction solution; removing water from the reaction solution; maintaining the reaction solution at a temperature of 205° C. to 330° C. and a pressure sufficient to prevent boiling for 10 minutes to 5 hours to form a product mixture comprising the polyetherimide and solvent; and isolating the polyetherimide.
-
公开(公告)号:US20200262977A1
公开(公告)日:2020-08-20
申请号:US16647924
申请日:2018-09-19
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Nitin Vilas Tople , Bernabe Quevedo Sanchez , Juan Justino Rodriguez Ordonez , Javier Nieves Remacha
IPC: C08G73/10
Abstract: A method of making a polyetherimide includes forming a monomer mixture comprising a bis(ether anhydride), a diamine and a volatile organic solvent; removing the volatile organic solvent to form a particulate solid; and melt polymerizing the particulate solid at a temperature 50 to 225° C. greater than the glass transition temperature of the polyetherimide in a single melt mixing device. The polyetherimide has an anhydride-amine stoichiometry and the standard deviation of anhydride-amine stoichiometry is less than 0.4 mol %.
-
-
-
-
-
-