1.
公开(公告)号:US20240286910A1
公开(公告)日:2024-08-29
申请号:US18586638
申请日:2024-02-26
发明人: Feng Shi , Fuzhou Song , Xiangyu Wang , Shuai LV , Yue Xu , Lingcui Zhang , Yan Shen , Jinbo Zhao
CPC分类号: C01B35/126 , H01B3/12 , C01P2002/72 , C01P2002/77 , C01P2004/03 , C01P2006/40
摘要: Disclosed are a borate MWDC with a low dielectric constant and a preparation method thereof by cold sintering. The method for preparing a borate MWDC with a low dielectric constant by cold sintering, including: subjecting a boron source and a metal source to first mixing to obtain a first mixture; subjecting the first mixture to presintering to obtain a presintered material; subjecting the presintered material and a boron oxide solution to second mixing to obtain a second mixture; and subjecting the second mixture to cold sintering to obtain the borate MWDC with the low dielectric constant.