    摘要: A connector includes a crimping portion (12) provided at an inner surface with projections (13) having inclined sides (19), the crimping portion (12) being provided with a combination of a base portion (14) and first and a second protruding portions (15) and (16) protruding from the base portion (14), the first protruding portion (15) having a distal end part (15a) located at an inside of a distal end part (16a) of the second protruding portion (16), the crimping portion (12) having a ring-shaped section perpendicular to a length direction of the aluminum electric wire (21), the projections (13) being projected into surface areas of the aluminum electric wire (21), with distorted regions formed along the inclined sides (19) in a surface part of the aluminum electric wire (21).

    Hot-dip Al-plated steel sheet and method for producing same

    公开(公告)号:US10760154B2

    公开(公告)日:2020-09-01

    申请号:US16083743

    申请日:2016-08-18

    IPC分类号: C23C2/12 C23C2/40 C22C21/00

    摘要: Provided is (i) a hot-dip Al-based alloy-coated steel sheet which includes a coated layer having a surface on which fine spangles are stably and sufficiently formed and which has a beautiful surface appearance due to the fine spangles thus formed on the surface of the coated layer, and (ii) a method of producing such a hot-dip Al-based alloy-coated steel sheet. The hot-dip Al-based alloy-coated steel sheet includes: a substrate steel sheet; and a hot-dip aluminum-based alloy coated layer which is formed on a surface of the substrate steel sheet and which contains boron at an average concentration of not less than 0.005 mass % and contains potassium at an average concentration of not less than 0.0004 mass %.

    Crimp terminal and electric wire with crimp terminal

    公开(公告)号:US09787003B2

    公开(公告)日:2017-10-10

    申请号:US14909897

    申请日:2013-08-08

    IPC分类号: H01R4/18 H01R4/62

    摘要: A crimp terminal includes an F-type crimp portion and a C-type crimp portion. The F-type crimp portion has first and second barrel tabs, preferably with an identical length, for crimping a tip end of a complex stranded wire. The F-type crimp portion is adapted to have distal ends of the first and second barrel tabs put together and pushed into the tip end of the complex stranded wire to be crimped. The C-type crimp portion has a third barrel tab for crimping the complex stranded wire. The third barrel tab is wound in a C-form on an outer periphery of the complex stranded wire to be crimped. The arrangement provides a crimp terminal and an electric wire with crimp terminal, that prevents or reduces increases in retained resistance at a crimp portion, and can also prevent an electric wire from slipping out of a crimp terminal.

    Method for producing molten Al plated steel wire

    公开(公告)号:US10957461B2

    公开(公告)日:2021-03-23

    申请号:US16214194

    申请日:2018-12-10

    摘要: A method of producing an Al plated steel wire comprises a first step of continuously immersing a material steel wire formed of a steel core into a molten Al plating bath and then withdrawing the material steel wire to a gas phase space. The material steel wire plated with a plating metal is brought into contact with a contact member at the plating bath rising portion to produce the Al plated steel wire, the Al plated steel wire having an average diameter DA (mm) and a minimum diameter DMIN (mm) in the longitudinal direction of the wire satisfying the following expression (1) (DA−DMIN)/DA≤0.10,  (1). The Al plated steel wire is then wound.

    HOT-DIP Al-PLATED STEEL SHEET AND METHOD FOR PRODUCING SAME

    公开(公告)号:US20190078189A1

    公开(公告)日:2019-03-14

    申请号:US16083743

    申请日:2016-08-18

    IPC分类号: C23C2/12 C23C2/40

    摘要: Provided is (i) a hot-dip Al-based alloy-coated steel sheet which includes a coated layer having a surface on which fine spangles are stably and sufficiently formed and which has a beautiful surface appearance due to the fine spangles thus formed on the surface of the coated layer, and (ii) a method of producing such a hot-dip Al-based alloy-coated steel sheet. The hot-dip Al-based alloy-coated steel sheet includes: a substrate steel sheet; and a hot-dip aluminum-based alloy coated layer which is formed on a surface of the substrate steel sheet and which contains boron at an average concentration of not less than 0.005 mass % and contains potassium at an average concentration of not less than 0.0004 mass %.