COATINGS, COMPOSITION AND METHOD RELATED TO NON-SPALLING LOW DENSITY HARDFACE COATINGS
    1.
    发明申请
    COATINGS, COMPOSITION AND METHOD RELATED TO NON-SPALLING LOW DENSITY HARDFACE COATINGS 有权
    涂料,组合物和方法相关的非膨胀低密度硬质涂料

    公开(公告)号:US20140134452A1

    公开(公告)日:2014-05-15

    申请号:US13799648

    申请日:2013-03-13

    Applicant: Mesocoat, Inc.

    Abstract: A heterogeneous composite body that is spall resistant and comprises a substantially discontinuous cermet phase in a substantially continuous metal rich matrix phase. The heterogeneous composite body is typically bonded to a substrate to form a hardfacing on the substrate. The heterogeneous composite body exhibits ductile phase toughening with a strain to failure of at least about 2 percent, a modulus of elasticity of less than about 35 million pounds per square inch, and a density of less than about 7 grams per cubic centimeter. The metal rich matrix phase between the ceramic rich regions in the heterogeneous composite body has an average minimum span of about 0.5 to 8 microns to allow ductility in the heterogeneous composite body. The heterogeneous composite body has a Vicker's hardness number of greater than approximately 500. The ceramic rich regions exhibit high hardness as compared with the matrix phase.

    Abstract translation: 一种异质复合体,其具有抗剥落性,并且在基本连续的富金属基质相中包含基本上不连续的金属陶瓷相。 非均相复合体通常结合到基底上以在基底上形成硬化面。 非均相复合体表现出韧性相增韧,破坏应变至少约为2%,弹性模量小于约3500万磅/平方英寸,密度小于约7克/立方厘米。 非均相复合体中陶瓷富集区之间的富金属基质相的平均最小跨度为约0.5至8微米,以允许非均相复合体中的延展性。 非均相复合体具有大于约500的维氏硬度值。与基体相相比,富陶瓷区显示出高的硬度。

    Coatings, composition and method related to non-spalling low density hardface coatings
    2.
    发明授权
    Coatings, composition and method related to non-spalling low density hardface coatings 有权
    与非剥落低密度硬质涂料相关的涂料,组成和方法

    公开(公告)号:US09376573B2

    公开(公告)日:2016-06-28

    申请号:US13799648

    申请日:2013-03-13

    Applicant: Mesocoat, Inc.

    Abstract: A heterogeneous composite body that is spall resistant and comprises a substantially discontinuous cermet phase in a substantially continuous metal rich matrix phase. The heterogeneous composite body is typically bonded to a substrate to form a hardfacing on the substrate. The heterogeneous composite body exhibits ductile phase toughening with a strain to failure of at least about 2 percent, a modulus of elasticity of less than about 35 million pounds per square inch, and a density of less than about 7 grams per cubic centimeter. The metal rich matrix phase between the ceramic rich regions in the heterogeneous composite body has an average minimum span of about 0.5 to 8 microns to allow ductility in the heterogeneous composite body. The heterogeneous composite body has a Vicker's hardness number of greater than approximately 500. The ceramic rich regions exhibit high hardness as compared with the matrix phase.

    Abstract translation: 一种异质复合体,其具有抗剥落性,并且在基本连续的富金属基质相中包含基本上不连续的金属陶瓷相。 非均相复合体通常结合到基底上以在基底上形成硬化面。 非均相复合体表现出韧性相增韧,破坏应变至少约为2%,弹性模量小于约3500万磅/平方英寸,密度小于约7克/立方厘米。 非均相复合体中陶瓷富集区之间的富金属基质相的平均最小跨度为约0.5至8微米,以允许非均相复合体中的延展性。 非均相复合体具有大于约500的维氏硬度值。与基体相相比,富陶瓷区显示出高的硬度。