公开(公告)号:US12065747B1
公开(公告)日:2024-08-20
申请号:US18609520
申请日:2024-03-19
Applicant: King Abdulaziz University
Inventor: Yasser A. Shaban , Shahed U. M. Khan , Mohamed Abdel Salam , Radwan Khalid Al-Farawati , Mohammed Ali Ghandourah , Doaa Fowzi Baamer , Mousa Zobidi
IPC: C25B11/031 , C25B1/04 , C25B9/17 , C25B11/061 , C25B11/077
CPC classification number: C25B11/031 , C25B1/04 , C25B11/061 , C25B11/077 , C25B9/17
Abstract: A method of generating oxygen including applying a potential of from 0.1 volts (V) to 2 V to an electrochemical cell and the electrochemical cell is at least partially submerged in an aqueous solution. On application of the potential, the aqueous solution is oxidized forming the oxygen. The electrochemical cell includes a counter electrode, and an electrocatalyst. The electrocatalyst includes a copper foam substrate and a nanocomposite. The nanocomposite includes iron oxide, cobalt oxide, and nickel oxide. Furthermore, particles of the nanocomposite are distributed on a surface of the copper foam substrate and the particles of the nanocomposite have a spherical shape with an average diameter of less than 500 nanometers (nm).