公开(公告)号:US07517405B2
公开(公告)日:2009-04-14
申请号:US11819474
申请日:2007-06-27
Applicant: Kap-Sok Yi
Inventor: Kap-Sok Yi
CPC classification number: C04B26/26 , B09B3/0033 , B09C1/08 , C04B2111/00732 , C04B2111/00767 , C08L95/005 , C09K17/40 , Y02W30/91 , Y02W30/93 , Y02W30/94 , Y02W30/95 , C04B18/0418 , C04B18/12 , C04B18/14 , C04B18/16 , C04B22/062 , C04B22/124 , C04B24/085 , C04B24/24 , C04B24/2676 , C04B24/36 , C08L53/02
Abstract: Disclosed herein is a composition for solidifying soil and industrial waste. The solidifying composition contains 16-24 wt % of straight asphalt, 0.06-0.10 wt % of an emulsifier for asphalt, 0.8-1.2 wt % of light oil, heavy oil or a mixture thereof, 0.01-0.03 wt % of calcium chloride, 0.8-1.2 wt % of lignin, 0.7-1.3 wt % of an acrylic emulsion-based asphalt modifier, 0.13-0.21 wt % of sodium hydroxide, 0.22-0.34 wt % of oleic acid, and the balance of water. A solidified material formed using this solidifying composition has increased density, strength and elasticity, improved durability and a short curing time. Furthermore, the solidifying composition enables soil and industrial waste to be recycled as a substitute for stone materials, such that it allows material sources to be readily secured in public or construction work fields, leading to a reduction in construction cost, and can also contribute to the preservation of the natural environment.
Abstract translation: 本文公开了一种用于固化土壤和工业废物的组合物。 固化组合物含有16-24重量%的直沥青,0.06-0.10重量%的沥青乳化剂,0.8-1.2重量%的轻油,重油或其混合物,0.01-0.03重量%的氯化钙,0.8 -1.2重量%的木质素,0.7-1.3重量%的丙烯酸乳液基沥青改性剂,0.13-0.21重量%的氢氧化钠,0.22-0.34重量%的油酸和余量的水。 使用这种凝固组合物形成的固化材料具有增加的密度,强度和弹性,改进的耐久性和短的固化时间。 此外,固化组合物可使土壤和工业废弃物作为石材的替代物,从而允许材料来源在公共或建筑工地上容易地固定,导致施工成本降低,并且还可以有助于 保护自然环境。