摘要:
The disclosed alloy has a temperature coefficient of electric resistance with an absolute value smaller than 100 ppm/.degree.C. in a temperature range between the order-disorder transformation point and melting point thereof, which alloy is made by molding an alloy consisting of 59.0-88.0 wt. % of palladium and the remainder of iron with a small amount of impurities, quenching the molded alloy from a temperature between the above-mentioned order-disorder transformation point and melting point to room temperature, cold working the quenched alloy for shaping, and annealing the shaped alloy.
摘要:
An electrical resistant alloy for use in a sensing coil having a small temperature dependence of electric resistance over a wide temperature range and a method of producing the same are disclosed. This alloy consists of 55.5 to 60.6 wt % of palladium and 44.5 to 39.4 wt % of silver and an inevitable amount of impurities, and has a temperature coefficient of electric resistance of .+-.20.times.10.sup.-6 /.degree.C. over a temperature range of -50.degree. C. to +730.degree. C.
摘要:
A rectangular hysteresis magnetic alloy consisting of 0.5-25 wt. % of Ta the balance of Fe and a rectangular hysteresis magnetic alloy consisting of 0.5-25 wt. % of Ta, 0.01-60 wt. % in total amount of at least one element selected from the group consisting of 0-10% of V, 0-0.5% of Nb, 0-35% of Cr, 0-20% of Mo, 0-20% of W, 0-25% of Ni, 0-25% of Cu, 0-40% of Co, 0-5% of Ti, 0-5% of Zr, 0-5% of Si, 0-10% of Al, 0-5% of Ge, 0-5% of Sn, 0-5% of Sb, 0-3% of Be, 0-15% of Mn, 0-2% of Ce and 0-1.5% of C, and the balance of Fe have an excellent rectangular hysteresis loop, a coercive force of more than 2 oerstads, excellent forgeability and workability, and are particularly suitable as a magnetic material for electromagnetic devices requiring rectangular hysteresis loop.
摘要:
The disclosed alloy has a temperature coefficient of electric resistance h an absolute value smaller than 100 ppm/.degree.C. in a temperature range between the order-disorder transformation point and melting point thereof, which alloy is made by molding an alloy consisting of 59.0-88.0 wt. % of palladium and the remainder of iron with a small amount of impurities, quenching the molded alloy from a temperature between the above-mentioned order-disorder transformation point and melting point to room temperature, cold working the quenched alloy for shaping, and annealing the shaped alloy.
摘要:
An electrical resistant alloy for use in a sensing coil having a small temperature dependence of electric resistance over a wide temperature range and a method of producing the same are disclosed. This alloy consists of 55.5 to 60.6 wt % of palladium and 44.5 to 39.4 wt % of silver and an inevitable amount of impurities, and has a temperature coefficient of electric resistance of .+-.20.times.10.sup.-6 /.degree.C. over a temperature range of -50.degree. C. to +730.degree. C.
摘要:
An electrical resistant alloy for use in a sensing coil having a small temperature dependence of electric resistance over a wide temperature range and a method of producing the same are disclosed. This alloy consists of 55.5 to 60.6 wt % of palladium and 44.5 to 39.4 wt % of silver and an inevitable amount of impurities, and has a temperature coefficient of electric resistance of .+-.20.times.10.sup.-6 /.degree.C. over a temperature range of -50.degree. C. to +730.degree. C.
摘要:
A rectangular hysteresis magnetic alloy consisting of 0.5-10 wt. % of Nb the balance of Fe and a rectangular hysteresis magnetic alloy consisting of 0.5-10 wt. % of Nb, 0.01-60 wt. % in total amount of at least one element selected from the group consisting of 0-10% of V, 0-25% of Ta, 0-25% of Cr, 0-20% of Mo, 0-10% of W, 0-30% of Ni, 0-20% of Cu, 0-45% of Co, 0-5% of Ti, 0-5% of Zr, 0-5% of Si, 0-5% of Al, 0-5% of Ge, 0-5% of Sn, 0-5% of Sb, 0-3% of Be, 0-15% of Mn, 0-2% of Ce and 0-1.5% of C, and the balance of Fe have an excellent rectangular hysteresis loop, a coercive force of more than 2 oersteds, excellent forgeability and workability and are particularly suitable as a magnetic material for electromagnetic devices requiring rectangular hysteresis loop.
摘要:
A wear-resistant alloy of high permeability having an effective permeabil of at least about 3,000 at 1 KHz, a saturation magnetic flux density of at least about 4,000 G, and a recrystallization texture of {110} +{311} is provided. The alloy is produced by cold working a forged or hot worked ingot of an alloy of a desired composition at a cold working ratio of at least about 50%, heating the cold worked alloy at a temperature which is below the m.p. of the alloy and not less than about 900.degree. C., and cooling the heated alloy from a temperature which is not less than an order-disorder transformation point (about 600.degree. C.) of the alloy. Alternatively, the alloy is produced by reheating the cooled alloy to a temperature which is not over than the order-disorder transformation point, and cooling the reheated alloy.
摘要:
A high damping capacity alloy comprising 1-45% by weight of Co and the remainder being Fe and, as the case may be, further comprising 0.01-30% in total, as an additional component, of at least one of Ni, Cr, Al, Cu, Mn, Sb, Nb, Mo, W, Ti, V, Ta, Si, Sn, Zn, Zr, C and Y, the alloy having high damping capacity more than 2.times.10.sup.-3, high cold workability and high corrosion resistance over wide temperature range.
摘要:
A high damping capacity alloy comprising of 0.1-95% by weight of Zn and the remainder of Al and, as the case may be, further comprising of 0.1-50% by weight in total of at least one subingredient of Sn, Pb, Sb, Ce, Cu Ta, Ni, Co, Fe, Nb, Zr, Si, Ti, Ca and B, the alloy having a damping capacity of not less than 6.times.10.sup.-3 after cold working with a reduction of area of at least 5%, and a process for producing the same.