Polymeric shaped articles
    1.
    发明授权
    Polymeric shaped articles 失效
    聚合物制品

    公开(公告)号:US4062826A

    公开(公告)日:1977-12-13

    申请号:US647890

    申请日:1976-01-09

    摘要: A shaped polymeric article of a gel-polymerisate of a homogeneous mixture comprisingA. from 5% to 95% by weight of polyurethane precursors comprising at least one polyfunctional compound and at least one polyisocyanate of the structure ##STR1## where X is a divalent radical, preferably --CH.sub.2 --, said precursors being capable of forming a cross-linked polyurethane having a glass-rubber transition temperature of at least 25.degree. C, preferably at least 35.degree. C, andB. from 95% to 5% by weight of cured polyester resin precursors, comprisingI. at least one ethylenically unsaturated polyester, andIi. at least one vinyl monomer.

    摘要翻译: 1.一种均匀混合物的凝胶聚合物的成型聚合物,其包含A.包含至少一种多功能化合物的聚氨酯前体的重量的5%至95%,以及至少一种结构单一的多晶型物(I),其中X是二价 自由基,优选-CH 2 - ,所述前体能够形成玻璃 - 橡胶转变温度至少为25℃,优选至少35℃和B的交联聚氨酯。从95重量%至5重量% 固化聚酯树脂前身,包括我至少一个乙烯基不饱和聚酯,和II。 最少一个乙烯单体。

    Shaped polymeric articles
    3.
    发明授权
    Shaped polymeric articles 失效
    成型聚合物制品

    公开(公告)号:US3962370A

    公开(公告)日:1976-06-08

    申请号:US506778

    申请日:1974-09-17

    摘要: A shaped polymeric article comprising from 1% to 60% by weight, preferably from 5% to 30% by weight of a cross-linked polymeric material having a glass-rubber transition temperature of not more than 25.degree.C and from 99% to 40% by weight, preferably from 95% to 70% by weight, of a vinyl polymer, in which the cross-linked polymeric material is formed from precursors therefor comprising at least one polymer, having a glass-rubber transition temperature of not more than 25.degree.C, at least 80% by weight of said polymer having a molecular weight of at least 3000, and preferably consisting of at least one polymer having a glass-rubber transition temperature of not more than 25.degree.C and a molecular weight of at least 3000, and at least on cross-linking agent reactive with said polymer.

    摘要翻译: 一种成型的聚合物制品,其包含1重量%至60重量%,优选5重量%至30重量%的玻璃 - 橡胶转变温度不超过25℃和99%至40%的交联聚合物材料 重量百分比,优选95%至70%的乙烯基聚合物,其中交联聚合物材料由其前体形成,其包含至少一种聚合物,其玻璃 - 橡胶转变温度不超过25 至少80重量%的分子量为至少3000的所述聚合物,并且优选由玻璃 - 橡胶转变温度不超过25℃至少分子量至少为一个的至少一种聚合物组成 3000,并且至少在与所述聚合物反应的交联剂上。

    Silicone elastomers
    5.
    发明授权
    Silicone elastomers 失效
    硅橡胶

    公开(公告)号:US3932555A

    公开(公告)日:1976-01-13

    申请号:US379315

    申请日:1973-07-16

    摘要: A reinforced silicone elastomer formed from 95% to 20% by weight of a cross-linkable poly(organo siloxane) and from 5% to 80% by weight of a polymerisable ethylenically unsaturated material by cross-linking a substantial proportion of the poly(organosiloxane) before a substantial proportion of the ethylenically unsaturated material is polymerised, the ethylenically unsaturated material subsequently being polymerised.

    摘要翻译: 通过交联相当比例的聚(有机硅氧烷)形成的95%-20%重量的可交联聚(有机硅氧烷)和5%至80%重量的可聚合烯属不饱和材料的增强硅氧烷弹性体 ),然后将烯键式不饱和材料的相当比例聚合,随后将烯属不饱和材料聚合。