摘要: The invention relates to coated effect pigments, wherein the coating comprises a binder which is suitable for powder paints. They comprise a crystalline and an amorphous fraction which is determined by C13 NMR MAS relaxation measurements, the relaxation of the 13C cores being fitted as a biexponential relaxation according to the formula (II) and the degree of crystallinity c being in a range between 40 to 85%, and relaxation having a short average relaxation time T1S and a long average relaxation time T1l, and T1l being in a range of from 65 to 130 s. The effect pigments coated according to the invention have at least one endothermic peak with a maximum from a range of Tmax=100 to 150° C. and an enthalpy ΔH associated with said peak from a range of 15 J/g to 80 J/g in DSC at a feed speed of 5° C./min, the enthalpy being calculated relative to the amount of the binder. The binders are applied to the effect pigment by way of spontaneous precipitation.
-
公开(公告)号:US20200181423A1
公开(公告)日:2020-06-11
申请号:US16089263
申请日:2017-03-30
申请人: ECKART GmbH
发明人: Burkhard Schreiber
IPC分类号: C09D5/03 , C09C1/00 , C09D5/36 , C09D167/02
摘要: The invention relates to coated effect pigments, wherein the coating comprises a binder which is suitable for powder paints. They comprise a crystalline and an amorphous fraction which is determined by C13 NMR MAS relaxation measurements, the relaxation of the 13C cores being fitted as a biexponential relaxation according to the formula (II) and the degree of crystallinity c being in a range between 40 to 85%, and relaxation having a short average relaxation time T1S and a long average relaxation time T1I, and T1I being in a range of from 65 to 130 s. The effect pigments coated according to the invention have at least one endothermic peak with a maximum from a range of Tmax=100 to 150° C. and an enthalpy ΔH associated with said peak from a range of 15 J/g to 80 J/g in DSC at a feed speed of 5° C./min, the enthalpy being calculated relative to the amount of the binder. The binders are applied to the effect pigment by way of spontaneous precipitation. M ( t , M 0 , a , c , T 1 s , T 1 l ) = M 0 · [ ( 1 - c ) · ( 1 - a · e - ( t T 1 s ) ) + c · ( 1 - a · e - ( t T 1 l ) ) ] ( II )
-
公开(公告)号:US10899934B2
公开(公告)日:2021-01-26
申请号:US16089263
申请日:2017-03-30
申请人: ECKART GmbH
发明人: Burkhard Schreiber
摘要: The invention relates to coated effect pigments, wherein the coating comprises a binder which is suitable for powder paints. They comprise a crystalline and an amorphous fraction which is determined by C13 NMR MAS relaxation measurements, the relaxation of the 13C cores being fitted as a biexponential relaxation according to the formula (II) and the degree of crystallinity c being in a range between 40 to 85%, and relaxation having a short average relaxation time T1S and a long average relaxation time T1I, and T1I being in a range of from 65 to 130 s. The effect pigments coated according to the invention have at least one endothermic peak with a maximum from a range of Tmax=100 to 150° C. and an enthalpy ΔH associated with said peak from a range of 15 J/g to 80 J/g in DSC at a feed speed of 5° C./min, the enthalpy being calculated relative to the amount of the binder. The binders are applied to the effect pigment by way of spontaneous precipitation. M ( t , M 0 , a , c , T 1 s , T 1 l ) = M 0 · [ ( 1 - c ) · ( 1 - a · e - ( t T 1 s ) ) + c · ( 1 - a · e - ( t T 1 l ) ) ] ( II )
-
公开(公告)号:US11702552B2
公开(公告)日:2023-07-18
申请号:US17123604
申请日:2020-12-16
申请人: ECKART GmbH
发明人: Burkhard Schreiber
IPC分类号: C09D5/36 , C09D5/03 , C09C1/00 , C09D167/02
CPC分类号: C09D5/032 , C09C1/0021 , C09D5/36 , C09D167/02 , C09C2200/1054 , C09C2200/406 , C09C2220/103 , C09D167/00 , C08K9/02
摘要: The invention relates to coated effect pigments, wherein the coating comprises a binder which is suitable for powder paints. They comprise a crystalline and an amorphous fraction which is determined by C13 NMR MAS relaxation measurements, the relaxation of the 13C cores being fitted as a biexponential relaxation according to the formula (II) and the degree of crystallinity c being in a range between 40 to 85%, and relaxation having a short average relaxation time T1S and a long average relaxation time T1l, and T1l being in a range of from 65 to 130 s. The effect pigments coated according to the invention have at least one endothermic peak with a maximum from a range of Tmax=100 to 150° C. and an enthalpy ΔH associated with said peak from a range of 15 J/g to 80 J/g in DSC at a feed speed of 5° C./min, the enthalpy being calculated relative to the amount of the binder. The binders are applied to the effect pigment by way of spontaneous precipitation.
-
公开(公告)号:US20230250298A1
公开(公告)日:2023-08-10
申请号:US18103033
申请日:2023-01-30
申请人: ECKART GmbH
发明人: Burkhard Schreiber
IPC分类号: C09D5/03 , C09C1/00 , C09D5/36 , C09D167/02
CPC分类号: C09D5/032 , C09C1/0021 , C09D5/36 , C09D167/02 , C09C2200/1054 , C09C2200/406 , C09C2220/103
摘要: The invention relates to coated effect pigments, wherein the coating comprises a binder which is suitable for powder paints. They comprise a crystalline and an amorphous fraction which is determined by C13 NMR MAS relaxation measurements, the relaxation of the 13C cores being fitted as a biexponential relaxation according to the formula (II) and the degree of crystallinity c being in a range between 40 to 85%, and relaxation having a short average relaxation time T1s and a long average relaxation time T1l, and T1l being in a range of from 65 to 130 s. The effect pigments coated according to the invention have at least one endothermic peak with a maximum from a range of Tmax=100 to 150° C. and an enthalpy ΔH associated with said peak from a range of 15 J/g to 80 J/g in DSC at a feed speed of 5° C./min, the enthalpy being calculated relative to the amount of the binder. The binders are applied to the effect pigment by way of spontaneous precipitation.
-
-
-
-