公开(公告)号:US20030084969A1
公开(公告)日:2003-05-08
申请号:US10192505
申请日:2002-07-11
Applicant: Daido Tokushuko Kabushiki Kaisha
Inventor: Kazuhiro Toyoda , Makoto Chujoya , Shigeo Hanajima , Takashi Suzuki , Takashi Orii , Takao Shimizu , Toshiharu Noda , Bunji Naito , Kohachiro Ohashi
IPC: C22C014/00
CPC classification number: B23K35/0261 , B23K35/325 , B23K35/40 , C23C4/131 , C23C26/02 , Y10S428/923 , Y10S428/925 , Y10T428/12458 , Y10T428/12993 , Y10T428/2951 , Y10T428/2953
Abstract: A Ti-base wire rod for forming molten metal excellent both in rod Seeding smoothness and arc stability is disclosed. A wire rod 301 is composed of Ti metal, and has in the surficial portion including the surface thereof an oxygen enriched layer having an oxygen concentration higher than that in an inner portion. Ratio Tw/Dw of the thickness Tw of the oxygen enriched layer and the diameter Dw of the wire rod is adjusted within a range from 1null10null3 to 1null10null1, and the average oxygen concentration of the oxygen enriched layer is adjusted to 1 wt % or above.
Abstract translation: 公开了一种用于形成熔融金属的钛基线材,其优良的棒种子平滑度和电弧稳定性。 线材301由Ti金属构成,在其表面的表面具有氧浓度高于内部氧浓度的氧浓缩层。 富氧层的厚度Tw与线材的直径Dw的比Tw / Dw在1×10 -3〜1×10 -1的范围内调整,将富氧层的平均氧浓度调整为1重量% %或以上。