METHOD OF TREATMENT OF A RUNNING FERROUS ALLOY SHEET AND TREATMENT LINE FOR ITS IMPLEMENTATION
    2.
    发明申请
    METHOD OF TREATMENT OF A RUNNING FERROUS ALLOY SHEET AND TREATMENT LINE FOR ITS IMPLEMENTATION 审中-公开
    处理运行中的合金板和处理线的方法进行实施

    公开(公告)号:US20150368730A1

    公开(公告)日:2015-12-24

    申请号:US14766326

    申请日:2013-02-06

    申请人: ARCELORMITTAL

    摘要: A method of treatment of a running ferrous alloy sheet containing at least one easily oxidized element is provided. The method includes a step of immersion of the sheet in a molten oxides bath.The molten oxides bath has a viscosity between 0.3.10−3 Pa·s and 3.10−1 Pa·s, the surface of the bath is contact with a non-oxidizing atmosphere, and the molten oxides are inert towards iron. The residence time of the running sheet in the bath is at least 1 s and the residues of oxides remaining on the surfaces of the sheet at the exit of the bath are eliminated.A treatment line of a ferrous alloy sheet for implementing the method, is provided. The treatment line includes a molten oxides bath having a viscosity between 0.3.10−3 and 3.10−1 Pa·s. The surface of the bath is contact with a non-oxidizing atmosphere, and the molten oxides are inert towards iron.Mechanical devices for eliminating the residues of molten oxides remaining on the surfaces of the ferrous alloy sheet are at the exit of the molten oxides bath.

    摘要翻译: 提供一种处理含有至少一种易氧化元素的运行中的铁合金板的方法。 该方法包括将片材浸入熔融氧化物浴中的步骤。 熔融氧化物浴的粘度为0.3×10 -3 Pa·s〜3.10〜1Pa·s,浴的表面与非氧化性气氛接触,熔融氧化物对铁呈惰性。 流动片在浴中的停留时间为至少1秒,并且消除了在浴的出口处残留在片材表面上的氧化物残留物。 提供了一种用于实施该方法的铁合金板的处理线。 处理线包括粘度在0.3.10-3和3.10-1Pa·s之间的熔融氧化物浴。 浴的表面与非氧化性气氛接触,并且熔融氧化物对铁是惰性的。 用于消除残留在铁合金板表面上的熔融氧化物残留物的机械装置在熔融氧化物浴的出口处。