摘要:
A method for producing an optical film is provided and includes: simultaneously coating at least two coating solutions over a transparent support, the at least two coating solutions each containing a solvent and a solute; and drying the solvent in each of the at least two coating solutions to provide at least two coating layers. When the at least two coating layers are 1, 2, . . . n−1 and n layers in sequence from the outermost surface of the at least two coating layers toward the transparent support, n being an integer of 2 or more, the main component of the solute in the n-th layer is insoluble or sparingly soluble in the main component of the solvent in the (n−1)-th layer.
摘要:
An optical film, which comprises: a transparent support; and an optical layer on or above the transparent support, wherein the optical layer contains a thickening agent which shows a viscosity of 10 mPa·sec or more when added to 2-butanone in a content of 3% by mass, and the optical layer has a thickness of 5 μm or more.
摘要:
A light-scattering film is provided and includes a transparent support having thereon at least a light-scattering layer. When substantially parallel light is incident on a surface of the film at an incident angle of 5°, the reflectance for an angle θ in the light-receiving part measured in a plane containing the film normal line and the incident direction is R(θ), the value obtained by normalizing R(θ) by the reflectance of regular reflection is Rrel(θ), and the value calculated from the maximum variation |dRrel(θ)/dθ|max for the angle θ is a scattering coefficient A (formula 1), the reflection coefficient B (formula 2) calculated from the scattering coefficient A and the 5° specular reflectance Rs is from 2.0 to 5.0. Scattering coefficient A=1/(10×|dRrel(θ)/dθ|max) (Formula 1) Reflection coefficient B=2.2×log 10(Rs)−7.5×log 10(A)+5.9 (Formula 2)
摘要:
An optical film, which comprises: a transparent support; and an optical layer on or above the transparent support, wherein the optical layer contains a thickening agent which shows a viscosity of 10 mPa·sec or more when added to 2-butanone in a content of 3% by mass, and the optical layer has a thickness of 5 μm or more.
摘要:
An optical film comprising a transparent support and a layer having internal scattering properties, wherein the optical film has an image sharpness, as measured in an optical comb width of 0.5 mm in conformity to JIS K7105, of from 30.0% to 99.9%, a haze value as caused by surface scattering of less than 3%, and a haze value as caused by internal scattering of from 15 to 40%.
摘要:
An anti-glare and anti-reflection film comprising: a transparent support; an anti-glare layer; and a low refractive index layer, wherein a value of haze which is caused due to internal scattering of the anti-glare and anti-reflection film is 0 to 35%, and a center line average roughness Ra of the anti-reflection film is 0.08 to 0.30 μm.
摘要:
An antireflection film includes, in a following order, a transparent substrate film; a medium refractive index layer; a high refractive index layer; and a low refractive index layer, wherein the medium refractive index layer is (A) a medium refractive index layer having a refractive index of 1.60 to 1.64 at a wavelength of 550 nm and a thickness of 55.0 to 65.0 nm, the high refractive index layer is (B) a high refractive index layer having a refractive index of 1.70 to 1.74 at a wavelength of 550 nm and a thickness of 105.0 to 115.0 nm, and the low refractive index layer is (C) a low refractive index layer having a refractive index of 1.32 to 1.37 at a wavelength of 550 nm and a thickness of 85.0 to 95.0 nm.
摘要:
Provided is an antireflection film including, in the following order: a transparent support; at least one antiglare layer or diffusive layer containing a transparent resin and light-transmissive resin particles; and a low-refractivity layer having a refractive index lower than that of any of the transparent support and the antiglare layer or diffusive layer, wherein the transparent resin is formed by curing a mixture containing (A) a polyfunctional (meth)acrylate having at least two (meth)acryloyl groups, and (B) a modified polyfunctional (meth)acrylate modified through addition of any of ethylene oxide, propylene oxide or caprolactone, and the light-transmissive resin particles contain (C) high-crosslinking light-transmissive particles which are so high-crosslinking as to have a residual monomer content of at most 2.0% and which have a compression strength of from 39 to 98 N/mm2.
摘要翻译:提供一种防反射膜,其按以下顺序包括:透明载体; 含有透明树脂和透光树脂颗粒的至少一个防眩层或扩散层; 和低折射率层,其折射率低于透明支撑体和防眩光层或扩散层的折射率,其中透明树脂通过固化含有(A)至少具有(A)的多官能(甲基)丙烯酸酯的混合物形成, 两个(甲基)丙烯酰基,和(B)通过添加环氧乙烷,环氧丙烷或己内酯中的任何一种而改性的改性多官能(甲基)丙烯酸酯,并且透光性树脂粒子含有(C)高交联性透光性粒子 其具有如此高交联度,其残留单体含量至多为2.0%,并且其压缩强度为39至98N / mm 2。
摘要:
An oil-in-water type emulsion coating composition having an aqueous phase and an oil phase, the oil-in-water type emulsion coating composition containing: an active energy ray-curable polyfunctional (meth)acrylate having three or more (meth)acryloyl groups within a molecule; and an organic solvent, in the oil phase, the organic solvent having a solubility of 30 g or less in 100 g of water and having a property capable of swelling or dissolving a substrate.
摘要:
An optical film, is provided, the optical film including: a support; and at least one antiglare layer having a surface that has asperities, wherein the at least one antiglare layer contains at least one kind of light transmitting particles including first light transmitting particles in an amount of 0.01 to 1 mass % based on a total solid content in the antiglare layer, the first light transmitting particles have an average particle size that is 0.1 to 4.0 μm greater than an average thickness of the antiglare layer, and a region θ(0.5) in which slope angles θ of the asperities of the surface of the antiglare layer lie within a range of 0°