公开(公告)号:US20090269582A1
公开(公告)日:2009-10-29
申请号:US12297138
申请日:2007-04-20
CPC分类号: D01F8/04 , Y10T428/2929
摘要: The present invention provides a process for producing a conjugate fiber that is excellent in strength, stretch elasticity, and transparency. The process includes a step (1) in which an elastomer resin (A) having stretching elasticity and an elastomer resin (B) having stretch elasticity, a permanent elongation of 25-70%, and a tensile elongation of 100-800% are separately melted and subjected to conjugate spinning using a conjugate spinneret having two nozzles so that the elastomer resin (A) forms a core and the elastomer resin (B) form a sheath; a step (2) in which the fiber obtained by composite spinning in the step (1) is heat-treated; and a step (3) in which the fiber heat-treated in the step (2) is stretched.
摘要翻译: 本发明提供强度,拉伸弹性和透明性优异的复合纤维的制造方法。 该方法包括步骤(1),其中具有拉伸弹性的弹性体树脂(A)和具有拉伸弹性的弹性体树脂(B),永久伸长率为25-70%,拉伸伸长率为100-800% 熔融并使用具有两个喷嘴的共轭喷丝头进行共轭纺丝,使得弹性体树脂(A)形成芯,并且弹性体树脂(B)形成鞘; 将在步骤(1)中通过复合纺丝获得的纤维进行热处理的步骤(2); 和步骤(3),其中在步骤(2)中热处理的纤维被拉伸。