摘要: The present invention relates to the use of a quaternary ammonium complex comprising at least one non-cyclic amide as a modifier for a creping adhesive used on a creping cylinder, e.g., a Yankee dryer.
摘要翻译: 本发明涉及包含至少一种非环酰胺作为改性剂的季铵络合物在起皱圆筒(例如扬克烘缸)上使用的起皱粘合剂的用途。
-
公开(公告)号:US5503713A
公开(公告)日:1996-04-02
申请号:US270088
申请日:1994-07-01
摘要: A process for making a cellulosic pulp fiber web having increased wet strength comprising the steps of: (1) adding to an aqueous cellulosic pulp fiber slurry a water soluble cationic polymer consisting of polydimethyldiallylammonium chloride to form a first treated slurry; (2) adding to the first treated slurry an aminopolyamide-epichlorohydrin acid salt resin solution having an E/N ratio of from about 0.6 to about 2.0 so that the weight percent of the cationic polymer is from about 1% to about 35% based on the weight of the resin, thus forming a second treated slurry; and (3) forming a cellulosic pulp fiber web by dewatering the second treated slurry.
摘要翻译: 一种制备具有增加的湿强度的纤维素纸浆纤维网的方法,包括以下步骤:(1)向纤维素浆浆纤维浆料中加入由聚二甲基二烯丙基氯化铵组成的水溶性阳离子聚合物以形成第一处理浆料; (2)向第一处理浆料中加入E / N比为约0.6至约2.0的氨基多胺 - 表氯醇酸盐树脂溶液,使得阳离子聚合物的重量百分比为约1%至约35%,基于 树脂的重量,从而形成第二处理浆料; 和(3)通过使第二处理浆料脱水而形成纤维素纸浆纤维网。
-
公开(公告)号:US20060207736A1
公开(公告)日:2006-09-21
申请号:US11081387
申请日:2005-03-15
申请人: Jeffery Boettcher , Nancy Clungeon , Hung Chou , Clay Ringold , Dexter Johnson
发明人: Jeffery Boettcher , Nancy Clungeon , Hung Chou , Clay Ringold , Dexter Johnson
IPC分类号: B31F1/12
CPC分类号: D21H21/146 , D21H17/10 , D21H17/52 , D21H17/55 , D21H25/005
摘要: An improved creping adhesive is prepared by first reacting a dibasic carboxylic acid, or its ester, half-ester, or anhydride derivative, with a polyalkylene polyamine, preferably in aqueous solution, under conditions suitable to produce a water soluble polyamide. The water-soluble polyamide is then reacted with an epihalohydrin until substantially fully cross-linked, and stabilized by acidification with phosphoric acid at the end of the polymerization reaction to form a water-soluble poly(aminoamide)-epihalohydrin creping adhesive that is re-wetable and facilitates water spray removal of buildup so as to lengthen the life of the creping blades, with attendant significant decrease in downtime and maintenance.
摘要翻译: 通过首先使二元羧酸或其酯,半酯或酸酐衍生物与聚亚烷基多胺反应,优选在水溶液中,在适于生产水溶性聚酰胺的条件下进行改性来制备改进的起皱粘合剂。 然后将水溶性聚酰胺与表卤代醇反应直到基本完全交联,并在聚合反应结束时用磷酸酸化稳定,形成水溶性聚(氨基酰胺) - 表卤醇起皱粘合剂, 可润湿并促进水喷雾去除,从而延长起皱刀片的使用寿命,同时显着降低停机时间和维护时间。
-
公开(公告)号:US20050245669A1
公开(公告)日:2005-11-03
申请号:US10833473
申请日:2004-04-28
申请人: Nancy Clungeon , Jeffrey Boettcher
发明人: Nancy Clungeon , Jeffrey Boettcher
IPC分类号: B31F1/12 , B31F1/14 , C09J133/26
CPC分类号: C09J133/26 , B31F1/14
摘要: A modified creping adhesive composition, comprising an adhesive component and at least one terpene modifier, and its use in the production of creped paper products by a process which includes the steps of adhering a paper web to the surface of a drying cylinder and separating the paper web from the drying cylinder with a creping blade.
摘要翻译: 一种改性起皱粘合剂组合物,其包含粘合剂组分和至少一种萜烯改性剂,以及其用于生产起皱纸产品的方法,该方法包括以下步骤:将纸幅粘附到干燥筒的表面并分离纸 带有起皱刀片的干燥筒的网。
-
公开(公告)号:US5575892A
公开(公告)日:1996-11-19
申请号:US461345
申请日:1995-06-05
摘要: A composition for improving the wet strength of cellulosic fibrous webs is comprised of an aminopolyamide-epichlorohydrin acid salt resin having an E/N ratio of from about 0.6 to about 2.0 and from about 1% to about 35% of a water soluble cationic polymer based on the weight of the resin. The composition has a total organic chlorine content of from about 0.5% to 1.0% by weight based on the weight of the aminopclyamide-epichlorohydrin acid salt resin.
摘要翻译: 用于改善纤维素纤维网的湿强度的组合物由具有约0.6至约2.0的E / N比和约1%至约35%的水溶性阳离子聚合物基的氨基多胺 - 表氯醇酸盐树脂 关于树脂的重量。 基于氨基酰胺 - 表氯醇酸盐树脂的重量,该组合物的总有机氯含量为约0.5重量%至1.0重量%。
-
公开(公告)号:US5435841A
公开(公告)日:1995-07-25
申请号:US248928
申请日:1994-05-25
IPC分类号: C08G12/12 , D21H19/62 , C09D7/12 , C09D103/02
摘要: This invention relates generally to insolubilizers for use with binders in paper coating compositions. There is provided a process for preparing both an insolubilizer and paper coating composition containing the insolubilizer and a binder which, when applied onto paper products, significantly enhances their wet-rub resistance.The insolubilizer is prepared by:(a) forming a glyoxal-urea adduct by reacting from about 1.0 to about 4.0 moles of glyoxal with about 1.0 mole of urea, at an elevated temperature,(b) cooling the glyoxal-urea adduct to room temperature,(c) adding from about 0.5 to about 2.0 moles of free glyoxal to the glyoxal-urea adduct to form an oligomer, and(d) adjusting the pH of the oligomer to from about 5 to about 7.
摘要翻译: 本发明一般涉及用于纸涂料组合物中的粘合剂的不溶性增稠剂。 提供了一种制备含有不溶物和粘合剂的不溶性和纸张涂料组合物的方法,当将其施加到纸产品上时,其显着增强了它们的耐湿摩擦性。 不溶物通过以下方法制备:(a)通过在高温下使约1.0至约4.0摩尔乙二醛与约1.0摩尔脲反应形成乙二醛 - 脲加合物,(b)将乙二醛 - 脲加合物冷却至室温 ,(c)从约0.5至约2.0摩尔的游离乙二醛加入到乙二醛 - 脲加合物中以形成低聚物,和(d)将低聚物的pH调节至约5至约7。
-
公开(公告)号:US07404875B2
公开(公告)日:2008-07-29
申请号:US10833473
申请日:2004-04-28
CPC分类号: C09J133/26 , B31F1/14
摘要: A modified creping adhesive composition, comprising an adhesive component and at least one terpene modifier, and its use in the production of creped paper products by a process which includes the steps of adhering a paper web to the surface of a drying cylinder and separating the paper web from the drying cylinder with a creping blade.
摘要翻译: 一种改性起皱粘合剂组合物,其包含粘合剂组分和至少一种萜烯改性剂,以及其用于生产起皱纸产品的方法,该方法包括以下步骤:将纸幅粘附到干燥筒的表面并分离纸 带有起皱刀片的干燥筒的网。
-
公开(公告)号:US5350796A
公开(公告)日:1994-09-27
申请号:US142642
申请日:1993-10-25
摘要: A composition for improving the wet strength of cellulosic fibrous webs is comprised of an aminopolyamide-epichlorohydrin acid salt resin having an E/N ratio of from about 0.6 to about 2.0 and from about 1% to about 35% of a water soluble cationic polymer based on the weight of the resin. The composition has a total organic chlorine content of from about 0.5% to 1.0% by weight based on the weight of the aminopolyamide-epichlorohydrin acid salt resin.
摘要翻译: 用于改善纤维素纤维网的湿强度的组合物由具有约0.6至约2.0的E / N比和约1%至约35%的水溶性阳离子聚合物基的氨基多胺 - 表氯醇酸盐树脂 关于树脂的重量。 该组合物的总有机氯含量为氨基聚酰胺 - 表氯醇酸盐树脂重量的约0.5%至1.0%。
-
-
-
-
-
-
-