METHOD FOR LEACHING COPPER OXIDE, REPLACING SULFURIC ACID WITH A NON-POLLUTING ORGANIC LEACHING AGENT
    1.
    发明申请
    METHOD FOR LEACHING COPPER OXIDE, REPLACING SULFURIC ACID WITH A NON-POLLUTING ORGANIC LEACHING AGENT 有权
    浸出氧化铜的方法,用非污染有机浸出剂代替硫酸

    公开(公告)号:US20130333524A1

    公开(公告)日:2013-12-19

    申请号:US13992376

    申请日:2011-11-28

    Abstract: The invention relates to a method for leaching copper oxide without using sulfuric acid, comprising the following steps consisting in: impregnating the copper oxide using a non-polluting organic leaching agent consisting of an aqueous solution formed by tricarboxylic acid (C6H807) combined with water in a mixture having an acidity varying between a pH of 1 and 5; obtaining copper citrate; and, optionally, again irrigating the copper oxide impregnated with the non-polluting organic leaching agent, thereby obtaining a more concentrated copper citrate.

    Abstract translation: 本发明涉及一种不使用硫酸浸出氧化铜的方法,包括以下步骤:使用由三羧酸(C6H807)与水组合形成的水溶液组成的无污染有机浸出剂浸渍氧化铜, 酸度在pH1和5之间变化的混合物; 获得柠檬酸铜; 并且可选地,再次冲洗浸渍有无污染有机浸出剂的氧化铜,从而获得更浓缩的柠檬酸铜。

    Method for leaching copper oxide, replacing sulfuric acid with a non-polluting organic leaching agent
    2.
    发明授权
    Method for leaching copper oxide, replacing sulfuric acid with a non-polluting organic leaching agent 有权
    浸出氧化铜的方法,用无污染的有机浸出剂代替硫酸

    公开(公告)号:US09206493B2

    公开(公告)日:2015-12-08

    申请号:US13992376

    申请日:2011-11-28

    Abstract: The invention relates to a method for leaching copper oxide without using sulfuric acid, comprising the following steps consisting in: impregnating the copper oxide using a non-polluting organic leaching agent consisting of an aqueous solution formed by tricarboxylic acid (C6H807) combined with water in a mixture having an acidity varying between a pH of 1 and 5; obtaining copper citrate; and, optionally, again irrigating the copper oxide impregnated with the non-polluting organic leaching agent, thereby obtaining a more concentrated copper citrate.

    Abstract translation: 本发明涉及一种不使用硫酸浸出氧化铜的方法,包括以下步骤:使用由三羧酸(C6H807)与水组合形成的水溶液组成的无污染有机浸出剂浸渍氧化铜, 酸度在pH1和5之间变化的混合物; 获得柠檬酸铜; 并且可选地,再次冲洗浸渍有无污染有机浸出剂的氧化铜,从而获得更浓缩的柠檬酸铜。