Zirconium based alloy of low irradiation growth, method of producing the
same, and use of the same
    5.
    发明授权
    Zirconium based alloy of low irradiation growth, method of producing the same, and use of the same 失效
    低辐照生长的锆基合金及其制造方法及其用途

    公开(公告)号:US5862194A

    公开(公告)日:1999-01-19

    申请号:US814337

    申请日:1997-03-11

    摘要: The present invention provides a zirconium based alloy member which has very small deformation of elongation and bow occurring due to irradiation growth, a method of manufacturing it, and particularly an channel box for an atomic reactor fuel assembly. A zirconium based alloy plate member having a width of not less than 100 mm and a long length, containing not more than 5 wt % Nb and/or not more 5 wt % Sn, the member having (0001) orientation (Fl value) of hexagonal Zr with respect to longitudinal direction ranging from 0.20 to 0.35, the difference in Fl between the middle and the end being not more than the value calculated from (0.0935.times.Fl-0.00585) and an amount of bow at neutron irradiation of 35 GWd/t which bow occurs in the channel box for a reactor being not more than 2.16 mm.

    摘要翻译: 本发明提供一种锆基合金构件,其由于照射生长而具有非常小的伸长变形和弓形,其制造方法,特别是用于原子反应堆燃料组件的通道箱。 一种宽度不小于100mm,长度不大于5重量%的Nb和/或不多于5重量%Sn的锆基合金板构件,具有(0001)取向(F1值)为 相对于纵向为0.20〜0.35的六方晶相,中间和末端之间的F1的差不大于由(0.0935xFl-0.00585)计算的值,中子照射下的弓的量为35GWd / t 在弯道出现弯道不大于2.16mm的反应堆。

    Method of producing a cladding tube for reactor fuel
    7.
    发明授权
    Method of producing a cladding tube for reactor fuel 失效
    生产反应堆燃料包层管的方法

    公开(公告)号:US4718949A

    公开(公告)日:1988-01-12

    申请号:US915555

    申请日:1986-10-06

    CPC分类号: G21C3/07 Y02E30/40 Y10S376/90

    摘要: A method of producing cladding tube comprises a step of temperature-gradient annealing in which the inner surface of the tube is heated to a temperature higher than the recrystallization temperature thereof, while the outer surface of the tube is cooled, after the tube has been hot-extruded. The temperature-gradient annealing is effected while a temperature gradient is maintained between the inner surface and the outer surface of the cladding tube. While keeping the inner surface at a temperature higher than the recrystallization temperature, and the outer surface at a temperature lower than the recrystallization temperature. The cladding tube is obtained with the outer surface which has an excellent resistance to nodular corrosion and a soft inner surface which has an excellent resistance to stress corrosion cracking.

    摘要翻译: 制造包层管的方法包括将管的内表面加热到高于其再结晶温度的温度的温度梯度退火步骤,同时管的外表面被冷却后,管被热 - 挤压。 在包覆管的内表面和外表面之间保持温度梯度的同时进行温度梯度退火。 同时将内表面保持在比再结晶温度高的温度,而外表面在低于再结晶温度的温度下。 获得具有优异的抗结块腐蚀性的外表面和具有优异的耐应力腐蚀开裂性的软内表面的包覆管。

    O-ethyl-S-propyl-dithiophosphoric acid phenyl or naphthyl esters
    8.
    发明授权
    O-ethyl-S-propyl-dithiophosphoric acid phenyl or naphthyl esters 失效
    O-乙基-S-丙基 - 二硫代磷酸苯基酯或萘基酯

    公开(公告)号:US3947529A

    公开(公告)日:1976-03-30

    申请号:US471082

    申请日:1974-05-17

    IPC分类号: C07F9/18 A01N9/36 C07F9/12

    CPC分类号: C07F9/18

    摘要: O-ethyl-S-n-propyl-dithiophosphoric acid phenyl or naphthyl esters, i.e. O-ethyl-S-n-propyl-O- or S- optionally substituted phenyl or naphthyl-phosphorothionothiol-- or dithiolates, of the formula ##EQU1## in which X is an oxygen or sulfur atom, andZ is a group of the formula ##SPC1##Y is a halogen atom or a lower alkyl, lower alkoxy, lower alkylmercapto, lower alkylsulfinyl, nitro, cyano or phenyl group, andm is 0, 1, 2 or 3, which possess insecticidal, acaricidal and nematocidal properties.

    摘要翻译: O-乙基-S-丙基 - 二硫代磷酸苯基或萘基酯,即O-乙基-S-丙基-O-或S-任选取代的苯基或萘基 - 硫代硫代硫代或二硫醇化物,其具有式S C2H5O(I)ANGLE PXZ nC 3H7S,其中X是氧或硫原子,Z是式Y的基团是卤素原子或低级烷基,低级烷氧基,低级烷基巯基,低级烷基亚磺酰基,硝基,氰基或苯基,M IS 0,1,2或3,哪些杀虫剂,杀虫剂和杀虫剂属性。