Process for making low density high resiliency flexible polyurethane foam
    1.
    发明授权
    Process for making low density high resiliency flexible polyurethane foam 有权
    制造低密度高弹性柔性聚氨酯泡沫的方法

    公开(公告)号:US08957123B2

    公开(公告)日:2015-02-17

    申请号:US13876620

    申请日:2010-12-07

    Abstract: A process for producing resilient, flexible polyurethane foams that function well in noise and vibration absorption applications for vehicle applications that are made from a blend of polyols (i) and an isocyanate (ii), wherein the blend of polyols (i) comprises a mixture of polyether polyols (i.a) that each has a hydroxyl equivalent weight of from 1200 to 3000 and at least 70% primary hydroxyl groups, from 5 to 80% by weight of the ethylene oxide-capped polypropylene oxides are nominally difunctional, from 0.5 to 20% by weight of the ethylene oxide-capped polypropylene oxides have a nominal functionality of four or higher, and the balance of the ethylene oxide-capped polypropylene oxides, but not less than 1.5% by weight thereof, are nominally trifunctional; an autocatalytic polyol (i.b) having a functionality in the range of 2 to 8 and a hydroxyl number in the range of 15 to 200, wherein said autocatalytic polyol compound comprising at least one tertiary amine group; and a low unsaturation polyol (i.c) having a functionality equal to or greater than 2, a hydroxyl equivalent weight of from 1800 to 2800, and a total unsaturation value of equal to or less than 0.06 meq/g.

    Abstract translation: 一种用于生产由多元醇(i)和异氰酸酯(ii)的共混物制成的车辆应用的噪声和振动吸收应用中良好的弹性,柔性聚氨酯泡沫体的方法,其中多元醇(i)的共混物包含混合物 的聚醚多元醇(ia),其各自具有1200至3000的羟基当量和至少70%的伯羟基,5至80重量%的环氧乙烷封端的聚环氧丙烷名义上为双官能的,为0.5至20 环氧乙烷封端的聚环氧丙烷的重量%具有四个或更高的标称官能度,其余的环氧乙烷封端的聚丙烯氧化物,但不小于1.5重量%,其名义上是三官能的; 官能度为2〜8,羟值在15〜200范围内的自催化多元醇(i.b),其中所述自催化多元醇化合物包含至少一个叔胺基团; 和低不饱和多元醇(i.c),其官能度等于或大于2,羟基当量为1800至2800,总不饱和度值等于或小于0.06meq / g。

    PROCESS FOR MAKING LOW DENSITY HIGH RESILIENCY FLEXIBLE POLYURETHANE FOAM
    2.
    发明申请
    PROCESS FOR MAKING LOW DENSITY HIGH RESILIENCY FLEXIBLE POLYURETHANE FOAM 有权
    制造低密度高弹性柔性聚氨酯泡沫的方法

    公开(公告)号:US20130184368A1

    公开(公告)日:2013-07-18

    申请号:US13876620

    申请日:2010-12-07

    Abstract: A process for producing resilient, flexible polyurethane foams that function well in noise and vibration absorption applications for vehicle applications that are made from a blend of polyols (i) and an isocyanate (ii), wherein the blend of polyols (i) comprises a mixture of polyether polyols (i.a) that each has a hydroxyl equivalent weight of from 1200 to 3000 and at least 70% primary hydroxyl groups, from 5 to 80% by weight of the ethylene oxide-capped polypropylene oxides are nominally difunctional, from 0.5 to 20% by weight of the ethylene oxide-capped polypropylene oxides have a nominal functionality of four or higher, and the balance of the ethylene oxide-capped polypropylene oxides, but not less than 1.5% by weight thereof, are nominally trifunctional; an autocatalytic polyol (i.b) having a functionality in the range of 2 to 8 and a hydroxyl number in the range of 15 to 200, wherein said autocatalytic polyol compound comprising at least one tertiary amine group; and a low unsaturation polyol (i.c) having a functionality equal to or greater than 2, a hydroxyl equivalent weight of from 1800 to 2800, and a total unsaturation value of equal to or less than 0.06 meq/g.

    Abstract translation: 一种用于生产由多元醇(i)和异氰酸酯(ii)的共混物制成的车辆应用的噪声和振动吸收应用中良好的弹性,柔性聚氨酯泡沫体的方法,其中多元醇(i)的共混物包含混合物 的聚醚多元醇(ia),其各自具有1200至3000的羟基当量和至少70%的伯羟基,5至80重量%的环氧乙烷封端的聚环氧丙烷名义上为双官能的,为0.5至20 环氧乙烷封端的聚环氧丙烷的重量%具有四个或更高的标称官能度,其余的环氧乙烷封端的聚丙烯氧化物,但不小于1.5重量%,其名义上是三官能的; 官能度为2〜8,羟值在15〜200范围内的自催化多元醇(i.b),其中所述自催化多元醇化合物包含至少一个叔胺基团; 和低不饱和多元醇(i.c),其官能度等于或大于2,羟基当量为1800至2800,总不饱和度值等于或小于0.06meq / g。