公开(公告)号:US20230287219A1
公开(公告)日:2023-09-14
申请号:US18012081
申请日:2021-06-21
发明人: Devin Schmitt
IPC分类号: C09C1/00
CPC分类号: C09C1/0015 , C01P2006/60 , C09C2200/301 , C09C2200/1054 , C09C2220/20
摘要: The present invention relates to an effect pigment having optically active layers consisting of a flake of a highly reflective material with directly adjacent on one side or on both sides a layer of a semiconducting material having a bandgap of 0.1 to 3.5 eV. The effect pigment may be further coated with a coating which is optically non-active in the visible wavelength region.
-
公开(公告)号:US20140154520A1
公开(公告)日:2014-06-05
申请号:US14147146
申请日:2014-01-03
发明人: James P. Rettker
CPC分类号: B22F1/00 , A61K8/0258 , A61K8/26 , A61K2800/437 , A61Q3/02 , B22F1/0055 , B22F3/26 , B22F9/04 , B22F9/16 , C09C1/62 , C09C1/64 , C09D5/38 , C09D11/037 , C23C4/185 , C23C26/00 , Y10T428/12014 , Y10T428/24901 , Y10T428/24917 , Y10T428/256 , Y10T428/2982
摘要: A process for preparing embossed fine particulate thin metal flakes having high levels of brightness and color intensity. The process comprises forming a release coat on a flexible polymeric carrier film, embossing the release coat with a diffraction grating pattern that is monoruled at an angle above 45°, vacuum metalizing the embossed release surface with a highly reflective metal such as aluminum, and solubilizing the metalized release coat in a solvent for removing the metal from the carrier to form embossed metal flakes that replicate the embossment pattern. The flakes are recovered from the solution containing the solvent and release coat polymer while avoiding high shear, particle sizing or other application of energy that would excessively break up the flakes, so that the D50 particle size of the flakes is maintained at or above 75 microns. The flakes have application to coatings and printing inks that produce extremely high brightness characterized as an optically apparent glitter or sparkle effect in combination with high color intensity or chromaticity.
摘要翻译: 一种用于制备具有高亮度和颜色强度水平的压花细颗粒薄金属薄片的方法。 该方法包括在柔性聚合物载体膜上形成剥离涂层,用以45度角度单一化的衍射光栅图案压印脱模涂层,用高反射金属如铝将真空金属化压花的脱模表面,并溶解 在用于从载体上除去金属的溶剂中的金属化脱模涂层以形成复制压花图案的压花金属片。 从含有溶剂和脱模涂层聚合物的溶液中回收薄片,同时避免高剪切,颗粒尺寸或其他施加能够过度分解薄片的能量,使得薄片的D50粒度保持在或高于75微米 。 薄片适用于产生极高亮度的涂料和印刷油墨,其特征在于具有高的色彩强度或色度的光学表观闪光或闪光效果。
-
公开(公告)号:US20130192789A1
公开(公告)日:2013-08-01
申请号:US13794959
申请日:2013-03-12
发明人: James P. Rettker , Bharat J. Adhia
CPC分类号: B22F1/00 , A61K8/0258 , A61K8/26 , A61K2800/437 , A61Q3/02 , B22F1/0055 , B22F3/26 , B22F9/04 , B22F9/16 , C09C1/62 , C09C1/64 , C09D5/38 , C09D11/037 , C23C4/185 , C23C26/00 , Y10T428/12014 , Y10T428/24901 , Y10T428/24917 , Y10T428/256 , Y10T428/2982
摘要: A process for preparing embossed fine particulate thin metal flakes having high levels of brightness and color intensity. The process comprises forming a release coat on a flexible polymeric carrier film, embossing the release coat with a diffraction grating pattern that is monoruled at an angle above 45°, vacuum metalizing the embossed release surface with a highly reflective metal such as aluminum, and solubilizing the metalized release coat in a solvent for removing the metal from the carrier to form embossed metal flakes that replicate the embossment pattern. The flakes are recovered from the solution containing the solvent and release coat polymer while avoiding high shear, particle sizing or other application of energy that would excessively break up the flakes, so that the D50 particle size of the flakes is maintained at or above 75 microns. The flakes have application to coatings and printing inks that produce extremely high brightness characterized as an optically apparent glitter or sparkle effect in combination with high color intensity or chromaticity.
摘要翻译: 一种用于制备具有高亮度和颜色强度水平的压花细颗粒薄金属薄片的方法。 该方法包括在柔性聚合物载体膜上形成剥离涂层,用以45度角度单一化的衍射光栅图案压印脱模涂层,用高反射金属如铝将真空金属化压花的脱模表面,并溶解 在用于从载体上除去金属的溶剂中的金属化脱模涂层以形成复制压花图案的压花金属片。 从含有溶剂和脱模涂层聚合物的溶液中回收薄片,同时避免高剪切,颗粒尺寸或其他施加能够过度分解薄片的能量,使得薄片的D50粒度保持在或高于75微米 。 薄片适用于产生极高亮度的涂料和印刷油墨,其特征在于具有高的色彩强度或色度的光学表观闪光或闪光效果。
-
-