公开(公告)号:US20060155098A1
公开(公告)日:2006-07-13
申请号:US11312886
申请日:2005-12-20
Applicant: Hermann Kauth , Wolfgang Ebert , Wilfried Haese , Helmut Einberger , Alexander Meyer , Andreas Frankenau , Uli Franz , Christian Eh , Stefaan De Vos , Bert Ruytinx
Inventor: Hermann Kauth , Wolfgang Ebert , Wilfried Haese , Helmut Einberger , Alexander Meyer , Andreas Frankenau , Uli Franz , Christian Eh , Stefaan De Vos , Bert Ruytinx
IPC: C08G64/00
CPC classification number: C08G64/24 , Y10T428/31507
Abstract: An improvement to the phase interface process of preparing aromatic polycarbonate is disclosed. The process is characterized in that the phosgenation is carried out at 0 to 40° C., and in that the temperature of the reaction mixture at the time of addition of the catalyst at 10 to 40° C., and in that the molar ratio of aromatic dihydroxy compounds to phosgene at 1:1.05 to 1:1.20. The polycarbonate thus produced is characterized in its low content of carbamates, making it particularly suitable for the preparation of optical storage media.
Abstract translation: 公开了制备芳族聚碳酸酯的相界面方法的改进。 该方法的特征在于光气化在0至40℃进行,并且在10至40℃下加入催化剂时反应混合物的温度,并且摩尔比 的芳族二羟基化合物与光气的比例为1:1.05至1:1.20。 由此制备的聚碳酸酯的特征在于其低含量的氨基甲酸酯,使其特别适用于制备光学存储介质。
-
公开(公告)号:US07705107B2
公开(公告)日:2010-04-27
申请号:US11312886
申请日:2005-12-20
Applicant: Hermann Kauth , Wolfgang Ebert , Wilfried Haese , Helmut Einberger , Alexander Meyer , Andreas Frankenau , Uli Franz , Christian Eh , Stefaan De Vos , Bert Ruytinx
Inventor: Hermann Kauth , Wolfgang Ebert , Wilfried Haese , Helmut Einberger , Alexander Meyer , Andreas Frankenau , Uli Franz , Christian Eh , Stefaan De Vos , Bert Ruytinx
CPC classification number: C08G64/24 , Y10T428/31507
Abstract: An improvement to the phase interface process of preparing aromatic polycarbonate is disclosed. The process is characterized in that the phosgenation is carried out at 0 to 40° C., and in that the temperature of the reaction mixture at the time of addition of the catalyst at 10 to 40° C., and in that the molar ratio of aromatic dihydroxy compounds to phosgene at 1:1.05 to 1:1.20. The polycarbonate thus produced is characterized in its low content of carbamates, making it particularly suitable for the preparation of optical storage media.
Abstract translation: 公开了制备芳族聚碳酸酯的相界面方法的改进。 该方法的特征在于光气化在0至40℃进行,并且在10至40℃下加入催化剂时反应混合物的温度,并且摩尔比 的芳族二羟基化合物与光气的比例为1:1.05至1:1.20。 由此制备的聚碳酸酯的特征在于其低含量的氨基甲酸酯,使其特别适用于制备光学存储介质。
-