REDUCED-CARBON FOOTPRINT CONCRETE COMPOSITIONS
    32.
    发明申请
    REDUCED-CARBON FOOTPRINT CONCRETE COMPOSITIONS 有权
    减少碳含量的混凝土组合物

    公开(公告)号:US20120000396A9

    公开(公告)日:2012-01-05

    申请号:US12838794

    申请日:2010-07-19

    IPC分类号: C04B14/26

    摘要: Reduced-carbon footprint concrete compositions, and methods for making and using the same, are provided. Aspects of the reduced-carbon footprint concrete compositions include CO2-sequestering carbonate compounds, which may be present in the hydraulic cement and/or aggregate components of the concrete. The reduced-carbon footprint concrete compositions find use in a variety of applications, including use in a variety of building materials and building applications.

    摘要翻译: 提供了减少碳足迹的混凝土组合物,以及制造和使用它们的方法。 减碳碳足迹混凝土组合物的方面包括CO 2截留的碳酸盐化合物,其可以存在于混凝土的水硬性水泥和/或骨料组分中。 减碳碳足迹混凝土组合物可用于各种应用,包括用于各种建筑材料和建筑应用中。

    Protective coatings and coating compositions
    33.
    发明授权
    Protective coatings and coating compositions 有权
    防护涂料和涂料组合物

    公开(公告)号:US07909923B2

    公开(公告)日:2011-03-22

    申请号:US12128136

    申请日:2008-05-28

    申请人: Norman V. Filbert

    发明人: Norman V. Filbert

    IPC分类号: C04B14/00 C04B14/26

    摘要: A protective coating on a metal surface comprises a particulate material produced by a method including heating an animal skeletal material to a temperature of at least 1000° C. for a time sufficient to convert at least part of the calcium carbonate in the skeletal material to calcium oxide and produce a calcined product; and then contacting at least part of the calcined product with water to produce the particulate material containing calcium hydrate.

    摘要翻译: 金属表面上的保护涂层包括通过包括将动物骨骼材料加热到至少1000℃的温度的方法产生的颗粒材料足以将至少部分骨骼材料中的碳酸钙转化为钙的时间 氧化并产生煅烧产物; 然后将至少部分煅烧产物与水接触以产生含有水合钙的颗粒材料。

    Grouting materials and their use
    35.
    发明授权
    Grouting materials and their use 失效
    灌浆材料及其用途

    公开(公告)号:US5707443A

    公开(公告)日:1998-01-13

    申请号:US505199

    申请日:1995-10-11

    摘要: A grouting material which is self-dispersing when brought into contact with a volume of water containing liquor or slurry and is settable to a solid mass after such dispersion, the material being in the form of self-dispersing granules or pellets and comprising a blend of component (A): a cementive constituent forming from 10 per cent to 95 per cent by weight of the composition; component (B): a dispersing constituent forming from 2 per cent to 75 per cent by weight of the composition; optional component (C): a swelling constituent which forms from 0 per cent to 50 per cent by weight of the composition; and component (D): a binder constituent which forms from 0.1 per cent to 10 per cent by weight of the composition; the percentages of components A, B, C and D adding to 100 per cent.

    摘要翻译: PCT No.PCT / GB94 / 01861 Sec。 371 1995年10月11日第 102(e)1995年10月11日的PCT PCT 1994年8月25日PCT公布。 第WO95 / 07887号公报 日期1995年3月23日一种当与一定体积的含有液体或浆料的水接触时自分散的灌浆材料,在分散后可固化成固体物质,该物质为自分散颗粒或颗粒形式 并且包含组分(A)的混合物:形成组合物重量的10%至95%的胶结成分; 组分(B):分散组分占组合物重量的2%至75%; 任选组分(C):一种溶胀成分,占组合物重量的0%至50%; 和组分(D):粘合剂组分,其占组合物重量的0.1%至10%; 组分A,B,C和D的百分比增加到100%。

    Additive composition with insulating, impermeabilizing and antishrink
properties
    36.
    发明授权
    Additive composition with insulating, impermeabilizing and antishrink properties 失效
    具有绝缘,不可渗透和抗收缩性能的添加剂组合物

    公开(公告)号:US5401310A

    公开(公告)日:1995-03-28

    申请号:US161518

    申请日:1993-12-06

    申请人: Antonio Ture

    发明人: Antonio Ture

    CPC分类号: C09D7/12 C04B22/10 C08K3/26

    摘要: New additive composition, in liquid or powder form, for thin slabs, plasters, concretes, prefabricated elements and refrectory elements, with insulating and impermeabilizing properties and with antishrink characteristics, comprising a bonding agent and an additive comprising a mixture of carbonates containing 59-75% CaCO.sub.3, 25-37% Si(CO.sub.3).sub.2, 0-2% Al.sub.2 (CO.sub.3).sub.3, 0-1% MgCO.sub.3 and 0-1% Fe.sub.2 (CO.sub.3).sub.3.

    摘要翻译: 新的添加剂组合物,液体或粉末形式,用于薄板,灰泥,混凝土,预制构件和重新起泡元件,具有绝缘和不稳定性能以及抗收缩特性,包括粘合剂和添加剂,其包含含有59-75 %CaCO3,25-37%Si(CO3)2,0-2%Al2(CO3)3,0-1%MgCO3和0-1%Fe2(CO3)3。