Abstract:
A process for synthesizing a Mn4+ doped phosphor includes contacting a precursor of formula I, at an elevated temperature with a fluorine-containing oxidizing agent in gaseous form to form the color stable Mn4+ doped phosphor; wherein A is Li, Na, K, Rb, Cs, or a combination thereof; M is Si, Ge, Sn, Ti, Zr, Al, Ga, In, Sc, Hf, Y, La, Nb, Ta, Bi, Gd, or a combination thereof; x is the absolute value of the charge of the [MFy] ion; y is 5, 6 or 7; and amount of Mn ranges from about 0.9 wt % to about 4 wt %, based on total weight.
Abstract:
A lighting apparatus is presented. The lighting apparatus includes a semiconductor light source, a color stable Mn4+ doped phosphor and a quantum dot material, each of the color stable Mn4+ doped phosphor and the quantum dot material being radiationally coupled to the semiconductor light source. A percentage intensity loss of the color stable Mn4| doped phosphor after exposure to a light flux of at least 20 w/cm2 at a temperature of at least 50 degrees Celsius for at least 21 hours is ≦4%. A backlight device including the lighting apparatus is also presented.
Abstract:
A process for synthesizing a Mn4+ doped phosphor includes contacting a precursor of formula I, Ax(M1−z,Mnz)Fy I at an elevated temperature with a fluorine-containing oxidizing agent in gaseous form to form the Mn4+ doped phosphor; wherein A is Li, Na, K, Rb, Cs, or a combination thereof; M is Si, Ge, Sn, Ti, Zr, Al, Ga, In, Sc, Hf, Y, La, Nb, Ta, Bi, Gd, or a combination thereof; x is the absolute value of the charge of the [MFy] ion; y is 5, 6 or 7; and 0.03≦z≦0.10.
Abstract:
A process for preparing a Mn4+ doped phosphor of formula I Ax[MFy]:Mn+4 I includes contacting a mixture of a compound of formula Ax[MFy], a compound of formula AX, and a Mn+n source comprising a fluoromanganese compound, with a fluorine-containing oxidizing agent in gaseous form, at an elevated temperature, to form the Mn4+ doped phosphor; wherein A is Li, Na, K, Rb, Cs, or a combination thereof; M is Si, Ge, Sn, Ti, Zr, Al, Ga, In, Sc, Hf, Y, La, Nb, Ta, Bi, Gd, or a combination thereof; X is F, Cl, Br, I, HF2, or a combination thereof; x is the absolute value of the charge of the [MFy] ion; y is 5, 6 or 7; and n is 2, 3, or 4.
Abstract:
A color stable Mn4+ doped phosphor of formula I, Ax[MFy]:Mn4+ I wherein A is Li, Na, K, Rb, Cs, or a combination thereof; M is Si, Ge, Sn, Ti, Zr, Al, Ga, In, Sc, Hf, Y, La, Nb, Ta, Bi, Gd, or a combination thereof; x is the absolute value of the charge of the [MFy] ion; y is 5, 6 or 7; and wherein % intensity loss of the phosphor after exposure to light flux of at least 80 w/cm2 at a temperature of at least 50° C. for at least 21 hours is ≦4%.
Abstract:
A process for synthesizing a color stable Mn4+ doped phosphor includes contacting a precursor of formula I, in gaseous form at an elevated temperature with a fluorine-containing oxidizing agent to form the color stable Mn4+ doped phosphor Ax[MFy]:Mn4+ I whereinA is Li, Na, K, Rb, Cs, NR4 or a combination thereof;M is Si, Ge, Sn, Ti, Zr, Al, Ga, In, Sc, Hf, Y, La, Nb, Ta, Bi, Gd, or a combination thereof;R is H, lower alkyl, or a combination thereof;x is the absolute value of the charge of the [MFy] ion; andy is 5, 6 or 7.
Abstract:
A color conversion film is provided. The film includes at least one narrow band emission phosphor dispersed within a binder matrix, wherein the narrow band emission phosphor has a D50 particle size from about 0.1 μm to about 15 μm and is selected from the group consisting of a green-emitting U6+-containing phosphor, a green-emitting Mn2+-containing phosphor, a red-emitting phosphor based on complex fluoride materials activated by Mn4+, and a mixture thereof. A device is also provided.
Abstract:
A color conversion film is provided. The film includes at least one narrow band emission phosphor dispersed within a binder matrix, wherein the narrow band emission phosphor has a D50 particle size from about 0.1 μm to about 15 μm and is selected from the group consisting of a green-emitting U6+-containing phosphor, a green-emitting Mn2+-containing phosphor, a red-emitting phosphor based on complex fluoride materials activated by Mn4+, and a mixture thereof. A device is also provided.
Abstract:
A lighting apparatus is presented. The lighting apparatus includes a semiconductor light source, a color stable Mn4+ doped phosphor and a quantum dot material, each of the color stable Mn4+ doped phosphor and the quantum dot material being radiationally coupled to the semiconductor light source. A percentage intensity loss of the color stable Mn4+ doped phosphor after exposure to a light flux of at least 20 w/cm2 at a temperature of at least 50 degrees Celsius for at least 21 hours is ≤4%. A backlight device including the lighting apparatus is also presented.