FAST FIRING METHOD FOR HIGH POROSITY CERAMICS
    11.
    发明申请
    FAST FIRING METHOD FOR HIGH POROSITY CERAMICS 有权
    高度陶瓷的快速燃烧方法

    公开(公告)号:US20150028527A1

    公开(公告)日:2015-01-29

    申请号:US13951802

    申请日:2013-07-26

    Abstract: A method for firing a green honeycomb ceramic body including heating the green honeycomb ceramic body from room temperature to a first temperature of about 300° C. The green honeycomb ceramic body is then heated from the first temperature to a second temperature of greater than or equal to about 800° C. at a heating rate of greater than or equal to about 90° C./hr. The green honeycomb ceramic body may have a diameter of from greater than or equal to about 4.0 inches to less than or equal to about 9.0 inches, and it may include a carbon-based pore former in a concentration of from greater than or equal to about 10% to less than or equal to about 45% by weight.

    Abstract translation: 一种焙烧生坯蜂窝陶瓷体的方法,包括将生坯蜂窝陶瓷体从室温加热至约300℃的第一温度。然后将生坯蜂窝陶瓷体从第一温度加热至大于或等于第二温度 至约800℃,加热速率大于或等于约90℃/小时。 绿色蜂窝陶瓷体可以具有大于或等于约4.0英寸至小于或等于约9.0英寸的直径,并且其可以包括浓度为大于或等于约的英寸的碳基成孔剂 10%至小于或等于约45重量%。

Patent Agency Ranking