公开(公告)号:US20180371597A1
公开(公告)日:2018-12-27
申请号:US16064195
申请日:2016-11-08
IPC分类号: C23C2/28 , C22C38/32 , C22C38/38 , C22C38/28 , C22C38/26 , C22C38/22 , C22C38/06 , C22C38/02 , C23C2/06 , C23C2/02 , C21D8/02
摘要: A high strength galvannealed steel sheet having, a) a composition consisting of the following elements (in wt. %): C 0.10-0.2 Mn 2.0-3.0 Si 0.2-0.5 Cr 0.1-0.7 Ti 0.01-0.07 Al≤0.2 Nb
-
公开(公告)号:US20220112586A1
公开(公告)日:2022-04-14
申请号:US17423742
申请日:2019-11-28
IPC分类号: C22C38/58 , C22C38/42 , C22C38/46 , C22C38/50 , C22C38/48 , C22C38/54 , C22C38/00 , C22C38/06 , C22C38/02 , C21D8/02
摘要: The invention relates to a cold rolled steel sheet having a composition consisting of (in wt. %): C 0.15-0.25; Si 0.5-1.6; Mn 2.2-2.8; Cr≤0.8; Mo≤0.2; Al 0.03-1.0; Nb≤0.04; V≤0.04; Ti 0.02-0.04; B 0.001-0.005; balance Fe apart from impurities, wherein the impurity contents of Cu and Ni are limited to ≤0.15, the cold rolled steel has a multiphase microstructure comprising a matrix of bainitic ferrite and ≤10 vol. % polygonal ferrite and the tensile strength (Rm) is 980-1500 MPa.
-
公开(公告)号:US20220112575A1
公开(公告)日:2022-04-14
申请号:US17423762
申请日:2019-11-28
IPC分类号: C21D9/52 , B32B15/01 , C22C38/58 , C22C38/54 , C22C38/50 , C22C38/42 , C22C38/06 , C22C38/02 , C22C38/00 , C21D8/04 , C21D6/00
摘要: A cold rolled steel strip or sheet has a composition consisting of (in wt. %): C 0.15-0.25; Si 0.5-1.6; Mn 2.2-3.2; Cr≤0.8; Mo≤0.2; Al 0.03-1.0; Nb≤0.04; V≤0.04; Ti 0.01-0.04; B 0.001-0.010; TUB 5-30; Cu≤0.15; Ni≤0.15; Ca≤0.01; balance Fe apart from impurities, where the cold rolled steel has a multiphase microstructure comprising a matrix mainly composed of tempered martensite and has a tensile strength (Rm) of at least 1380 MPa.
-
公开(公告)号:US20220010827A1
公开(公告)日:2022-01-13
申请号:US17289569
申请日:2019-11-28
摘要: A resistance spot welded joint of at least two steel sheets and a method of producing a resistance spot welded joint of at least two steel sheets, wherein at least one of the steel sheets is provided with a Zn containing layer, the steel sheet has a tensile strength of at least 980 MPa, a multiphase microstructure comprising bainite, bainitic ferrite and tempered martensite in a total amount of at least of 75 volume % and retained austenite in an amount of 3-20 volume % and wherein the steel sheet provided with the Zn containing layer has a composition consisting of (in wt. %): C 0.1-0.3; Si 0.2-3.0; Mn 1.0-3.0; Cr≤2.0; Mo≤0.5; Al≤2.0; Nb≤0.2; V≤0.2; Ti 0.01-0.15; B 0.0005-0.01; and balance Fe apart from impurities, wherein the heat affected zone in the spot welded joint is free from cracks having a length of more than 500 μm.
-
公开(公告)号:US20190352750A1
公开(公告)日:2019-11-21
申请号:US16461689
申请日:2017-11-24
摘要: A high strength cold rolled steel sheet has a composition consisting of the following elements (in wt. %): C 0.07-0.15, Mn 2.3-3.2, Si 0.6-1.2, Cr 0.05-0.5, Al≤0.2 Nb≤0.1, balance Fe apart from impurities, a multiphase microstructure comprising a matrix of bainitic ferrite, and a tensile strength (Rm) of 980-1100 MPa.
-
-
-
-