Wear-resistant sintered ferrous alloy and method of producing same
    1.
    发明授权
    Wear-resistant sintered ferrous alloy and method of producing same 失效
    耐磨烧结铁合金及其制造方法

    公开(公告)号:US4561889A

    公开(公告)日:1985-12-31

    申请号:US545245

    申请日:1983-10-25

    摘要: A sintered ferrous alloy which is high in wear resistance and relatively weak in the tendency to abrade another metal material with which the sintered alloy makes rubbing contact and suitable for rocker arm tips in automotive engines for example. The sintered alloy is produced by compacting and sintering a powder mixture of 15-50 parts by weight of a Fe-Cr-B alloy powder, which contains 10-35% of Cr and 1.0-2.5% of B, 1.0-3.5 parts by weight of graphite powder, such an amount of a Cu-P alloy powder that the powder mixture contains 0.2-1.5% of P and 1.0-20.0% of Cu and the balance of an iron powder.

    摘要翻译: 一种烧结铁合金,其耐磨性高,并且相对较弱的倾向于研磨另一种金属材料,烧结合金与其摩擦接触并适用于例如汽车发动机中的摇臂尖。 烧结合金是通过将15〜50重量份的Fe-Cr-B合金粉末进行压实和烧结来制造的,所述Fe-Cr-B合金粉末含有10-35%的Cr和1.0-2.5%的B,1.0-3.5份的 石墨粉的重量,这种量的Cu-P合金粉末,粉末混合物含有0.2-1.5%的P和1.0-20.0%的Cu,余量为铁粉。

    Wear-resistant sintered ferrous alloy and method of producing same
    2.
    发明授权
    Wear-resistant sintered ferrous alloy and method of producing same 失效
    耐磨烧结铁合金及其制造方法

    公开(公告)号:US4504312A

    公开(公告)日:1985-03-12

    申请号:US506767

    申请日:1983-06-22

    CPC分类号: C22C33/0207 C22C33/0257

    摘要: A highly wear-resistant sintered ferrous alloy which consists essentially of 2.0-8.0% of Cr, 0.1-1.0% of B, 1.0-2.5% of Si, 0.3-1.2% of Mn, 1.2-3.8% of C, by weight, and the balance of Fe. The alloy is produced by compacting and sintering a powder mixture, which is preferably prepared by mixing 75-90 parts by weight of a cast iron powder with 25-10 parts by weight of a Fe--Cr--B--Si alloy powder.

    摘要翻译: 一种高度耐磨的烧结铁合金,其基本上由2.0%至6.0%的Cr,0.1-1.0%的B,1.0-2.5%的Si,0.3-1.2%的Mn,1.2-3.8%的C, 余量为Fe。 该合金通过压制和烧结粉末混合物来制备,该混合物优选通过将75-90重量份的铸铁粉末与25-10重量份的Fe-Cr-B-Si合金粉末混合而制备。