公开(公告)号:US20240237482A1
公开(公告)日:2024-07-11
申请号:US18491334
申请日:2023-10-20
Applicant: Samsung Display Co., Ltd.
Inventor: JAEHO LEE , JUN HAK OH , JEONG SEOK LEE
CPC classification number: H10K59/871 , C03B32/02 , C03C10/00 , C03C10/0027 , C03C15/00 , C03C21/002 , H05K5/03 , C03C2204/00
Abstract: A window includes a glass substrate having a plurality of first portions and a plurality of second portions. The plurality of first and second portions are alternately arranged with each other along a first direction. An upper surface of each of the plurality of first portions includes a first depressed pattern of a plurality of first depressed patterns defined therein. A first length in the first direction of each of the plurality of first depressed patterns is in a range of about 20 nm to about 2000 nm. A crystal content of each of the plurality of second portions is greater than a crystal content of each of the plurality of first portions.
-
公开(公告)号:US20230312411A1
公开(公告)日:2023-10-05
申请号:US18098941
申请日:2023-01-19
Applicant: Samsung Display Co., Ltd.
Inventor: TAEHO AN , JEONG SEOK LEE , JUN HAK OH , SOOKKYUNG YOU , HYUN-IL CHO
IPC: C03C21/00
CPC classification number: C03C21/002 , C03C2203/52
Abstract: A method of manufacturing a window, includes: preparing a first preliminary glass substrate that does not contain Li+ ions and contains Na+ ions; providing a first strengthening molten salt to the first preliminary glass substrate to form a second preliminary glass substrate; providing heat to the second preliminary glass substrate at a temperature of about 400 to 500° C. for a period of about 3 to 7 hours to form a third preliminary glass substrate; and providing a second strengthening molten salt to the third preliminary glass substrate to form a window.
-