FILLER REINFORCED THERMOPLASTIC COMPOSITIONS WITH IMPROVED BONDING STRENGTH
    1.
    发明申请
    FILLER REINFORCED THERMOPLASTIC COMPOSITIONS WITH IMPROVED BONDING STRENGTH 审中-公开
    具有改善粘结强度的填料增强热塑性组合物

    公开(公告)号:US20170029615A1

    公开(公告)日:2017-02-02

    申请号:US15303567

    申请日:2015-06-23

    Abstract: Disclosed herein are blended thermoplastic compositions and methods relating to the same. In an aspect, a composition can comprise from about 20 wt % to about 90 wt % of a polybutylene terephthalate component; a second component comprising one or more of: from greater than about 0 wt % to about 40 wt % of a polyester component, from greater than about 0 wt % to about 30 wt % of a resorcinol-based aryl polyester component having greater than or equal to 40 mole % of its moieties derived from resorcinol, from greater than about 0 wt % to about 30 wt % of a polyetherimide component, and from greater than about 0 wt % to about 30 wt % of a polycarbonate component; from about 10 wt % to about 60 wt % of a filler component.

    Abstract translation: 本文公开了混合的热塑性组合物和与其相关的方法。 在一方面,组合物可以包含约20重量%至约90重量%的聚对苯二甲酸丁二醇酯组分; 第二组分,其包含以下组分中的一种或多种:大于约0重量%至约40重量%的聚酯组分,大于约0重量%至约30重量%的间苯二酚基芳基聚酯组分,其具有大于或 等于其间
    苯二酚部分的40摩尔%,聚醚酰亚胺组分大于约0重量%至约30重量%,聚碳酸酯组分大于约0重量%至约30重量% 约10重量%至约60重量%的填料组分。

    GLASS-REINFORCED PDMS COPOLYCARBONATE RESINS

    公开(公告)号:US20190002652A1

    公开(公告)日:2019-01-03

    申请号:US15746589

    申请日:2016-07-29

    Abstract: A thermoplastic composition including a resin phase and 10% to 55%, especially 25% to 45% of glass fibers by weight of the composition is disclosed. The resin phase includes a polysiloxane block copolymer including polydimethylsiloxane blocks and polycarbonate blocks derived from bisphenol A. The resin phase further includes a polycarbonate and has between 2.0 wt % and 10 wt % by weight of siloxane. The thermoplastic composition has (i) a notched Izod impact strength of at least 150 Joules per meter measured at 23° C. according to ASTM D256, (ii) a tensile strength greater than 95 MPa as determined by ASTM D638, (iii) a tensile modulus greater than 10,900 MPa as determined by ASTM D638 and (iv) an unnotched Izod impact strength greater than 775 Joules per meter measured at 23° C. according to ASTM D256.

    REFLECTIVE ARTICLES AND METHOD OF MANUFACTURING

    公开(公告)号:US20180299101A1

    公开(公告)日:2018-10-18

    申请号:US15526435

    申请日:2015-11-05

    Inventor: Wei ZHAO Xiaoyu SUN

    Abstract: A reflective article includes a reflector and a light source. The reflector includes a polymer layer having a first side configured to house a light source, and an opposite second side, and a metal layer disposed on the opposite second side of the polymer layer. The light source is located adjacent to the first side of the polymer layer. A method of making the reflective article is provided, including providing the above-described reflector, and locating a light source adjacent to the first side of the polymer layer. A method of making the reflector is also provided, including providing the polymer layer having a first side configured to house a light source, and an opposite second side, and metallizing at least a portion of the second side. The reflective article is useful for mobile electronic devices.