发明授权
- 专利标题: Spot welded joint
- 专利标题(中): 点焊接头
-
申请号: US13390493申请日: 2010-08-30
-
公开(公告)号: US08962149B2公开(公告)日: 2015-02-24
- 发明人: Hatsuhiko Oikawa , Hideki Hamatani , Masafumi Azuma , Noriyuki Suzuki , Fuminori Watanabe , Naoki Maruyama , Hiroyuki Kawata
- 申请人: Hatsuhiko Oikawa , Hideki Hamatani , Masafumi Azuma , Noriyuki Suzuki , Fuminori Watanabe , Naoki Maruyama , Hiroyuki Kawata
- 申请人地址: JP Tokyo
- 专利权人: Nippon Steel & Sumitomo Metal Corporation
- 当前专利权人: Nippon Steel & Sumitomo Metal Corporation
- 当前专利权人地址: JP Tokyo
- 代理机构: Birch, Stewart, Kolasch & Birch, LLP
- 优先权: JP2009-199908 20090831; JP2009-272076 20091130; JP2010-106442 20100506; JP2010-173929 20100802
- 国际申请: PCT/JP2010/064748 WO 20100830
- 国际公布: WO2011/025015 WO 20110303
- 主分类号: B32B15/01
- IPC分类号: B32B15/01 ; B32B15/04 ; B32B15/18 ; B23K11/11 ; C22C38/00 ; C22C38/02 ; C22C38/04 ; C22C38/06 ; B23K11/16
摘要:
Provided is a spot welded joint (10) which includes at least one thin steel plate with a tensile strength of 750 MPa to 1850 MPa and a carbon equivalent Ceq of equal to or more than 0.22 mass % to 0.55 mass % and in which a nugget (3) is formed in an interface of the thin steel plates (1A, 1B). In a nugget outer layer zone, a microstructure consists of a dendrite structure in which an average value of arm intervals is equal to or less than 12 μm, an average grain diameter of carbides contained in the microstructure is 5 nm to 100 nm, and a number density of carbides is equal to or more than 2×106/mm2.
公开/授权文献
- US20120141829A1 SPOT WELDED JOINT AND SPOT WELDING METHOD 公开/授权日:2012-06-07
信息查询