发明授权
- 专利标题: Steel product with a high austenite grain coarsening temperature
- 专利标题(中): 钢产品具有高奥氏体晶粒粗化温度
-
申请号: US11255604申请日: 2005-10-20
-
公开(公告)号: US07485196B2公开(公告)日: 2009-02-03
- 发明人: Walter N. Blejde , Rama Ballav Mahapatra , James Geoffrey Williams , Frank Barbaro , Philip John Renwick , Harold Roland Kaul , Andrew Phillips , Christopher Ronald Killmore , Lazar Strezov
- 申请人: Walter N. Blejde , Rama Ballav Mahapatra , James Geoffrey Williams , Frank Barbaro , Philip John Renwick , Harold Roland Kaul , Andrew Phillips , Christopher Ronald Killmore , Lazar Strezov
- 申请人地址: US NC Charlotte
- 专利权人: Nucor Corporation
- 当前专利权人: Nucor Corporation
- 当前专利权人地址: US NC Charlotte
- 代理机构: Hahn Loeser & Parks, LLP
- 主分类号: C22C38/00
- IPC分类号: C22C38/00
摘要:
A steel product with a high austenite grain coarsening temperature having less than 0.4% carbon, less than 0.06% aluminium, less than 0.01% titanium, less than 0.01% niobium, and less than 0.02% vanadium by weight, and having fine oxide particles containing silicon and iron distributed through the steel microstructure having an average particle size less than 50 nanometers and may be between 5 and 30 nanometers. The steel product may have fine oxide particles distributed through the microstructure capable of restricting ferrite recrystallisation for strain levels up to at least 10.0%, for temperatures up to 750° C. with holding times up to 20 minutes. The steel product may be made by continuous casting of steel strip introduced between the casting rolls to form a casting pool of molten carbon steel having a total oxygen content of at least 70 ppm usually less than 250 ppm, and a free oxygen content 20 and 60 ppm, counter rotating the casting rolls.