SEMICONDUCTOR CHAMBER COATINGS AND PROCESSES
Abstract:
Systems and methods may be used to produce coated components. Exemplary semiconductor chamber components may include an aluminum alloy comprising nickel and may be characterized by a surface. The surface may include a corrosion resistant coating. The corrosion resistant coating may include a conformal layer and a non-metal layer. The conformal layer may extend about the semiconductor chamber component. The non-metal oxide layer may extend over a surface of the conformal layer. The non-metal oxide layer may be characterized by an amorphous microstructure having a hardness of from about 300 HV to about 10,000 HV. The non-metal oxide layer may also be characterized by an sp2 to sp3 hybridization ratio of from about 0.01 to about 0.5 and a hydrogen content of from about 1 wt. % to about 35 wt. %.