公开(公告)号:US12005687B2
公开(公告)日:2024-06-11
申请号:US18171925
申请日:2023-02-21
Applicant: SCHOTT AG
Inventor: Armin Vogl , Thomas Schmiady , Thilo Zachau , Jochen Alkemper , Michael Meister , Christian Kunert , Lutz Klippe , Rüdiger Dietrich
IPC: B32B3/26 , B32B3/02 , B32B3/30 , B32B17/00 , B32B17/10 , C03B17/06 , C03B18/02 , C03B23/023 , C03C3/04 , C03C3/083 , C03C3/087 , C03C3/093 , C03C21/00
CPC classification number: B32B3/263 , B32B3/02 , B32B3/26 , B32B3/30 , B32B17/10036 , B32B17/10045 , B32B17/10119 , B32B17/10137 , C03B17/064 , C03B18/02 , C03B23/023 , C03C3/083 , C03C3/087 , C03C3/093 , C03C21/002 , B32B2315/08 , B32B2329/04 , B32B2329/06 , B32B2551/00 , B32B2571/00 , B32B2605/006 , Y10T428/24777
Abstract: A thin glass substrate, as well as a method and an apparatus are provided. The glass substrate has a glass having first and second main surfaces and elongated elevations on one of the main surfaces. The elevations rise in a normal direction, have a longitudinal extent that is greater than two times a transverse extent, and have a height, on average, that is less than 100 nm, and with a transverse extent of the elevation smaller than 40 mm. The method includes melting a glass, hot forming the glass, and adjusting a viscosity of the glass so that for the viscosity η1 for a first stretch over a first distance of up to 1.5 m downstream of a flow rate control component and y1 indicating a second distance to a location immediately downstream the flow rate control component the equation lg η1(y1)/dPa·s=(lg η01/dPa·s+a1(y1)) applies.
-
公开(公告)号:USRE49895E1
公开(公告)日:2024-04-02
申请号:US17526434
申请日:2021-11-15
Applicant: SCHOTT AG
Inventor: Michael Schwall , Christian Mix , Jochen Alkemper , Peter Thomas
Abstract: A thermally tempered glass element is provided made of glass with two opposite faces that are under compressive stress of at least 40 MPa. The glass has a working point at which the glass has a viscosity of 104 dPa·s of at most 1350° C. The glass has a viscosity versus temperature profile and a coefficient of thermal expansion versus temperature profile of the glass are such that a variable (750° C.-T13)/(CTELiq-CTEsSol) has a value of at most 5*106 K2. The CTELiq is a coefficient of linear thermal expansion of the glass above a glass transition temperature Tg, the CTESol is a coefficient of linear thermal expansion of the glass in a temperature range from 20° C. to 300° C., and the T13 is a temperature at which the glass has a viscosity of 1013 dPa·s.
-
公开(公告)号:US11745459B2
公开(公告)日:2023-09-05
申请号:US16851998
申请日:2020-04-17
Applicant: SCHOTT AG
Inventor: Armin Vogl , Thomas Schmiady , Thilo Zachau , Michael Meister , Jochen Alkemper , Christian Kunert , Lutz Klippe , Rüdiger Dietrich
IPC: C03C3/083 , C03B17/06 , C03B18/02 , C03C3/087 , C03C3/093 , B32B3/26 , B32B17/10 , B32B3/30 , B32B3/02 , C03C21/00 , C03B23/023
CPC classification number: B32B3/263 , B32B3/02 , B32B3/26 , B32B3/30 , B32B17/10036 , B32B17/10045 , B32B17/10119 , B32B17/10137 , C03B17/064 , C03B18/02 , C03B23/023 , C03C3/083 , C03C3/087 , C03C3/093 , C03C21/002 , B32B2315/08 , B32B2329/04 , B32B2329/06 , B32B2551/00 , B32B2571/00 , B32B2605/006 , Y10T428/24777
Abstract: Thin glass substrates are provided. Also provided are methods and apparatuses for the production thereof and provides a thin glass substrate of improved optical quality. The method includes, after the melting and before a hot forming process, adjusting the viscosity of the glass that is to be formed or has at least partially been formed is in a defined manner for the thin glass substrate to be obtained. The apparatus includes a device for melting, a device for hot forming, and also a device for defined adjustment of the viscosity of the glass to be formed into a thin glass substrate, and the device for defined adjustment of the viscosity of the glass to be formed into a thin glass substrate is arranged upstream of the device for hot forming.
-
公开(公告)号:US11993062B2
公开(公告)日:2024-05-28
申请号:US16450419
申请日:2019-06-24
Applicant: SCHOTT AG
Inventor: Jochen Alkemper , Lutz Klippe , Rüdiger Dietrich
IPC: B32B17/10 , B32B3/02 , B32B3/26 , B32B3/30 , C03B17/06 , C03B18/02 , C03B23/023 , C03C3/083 , C03C3/087 , C03C3/093 , C03C21/00
CPC classification number: B32B3/263 , B32B3/02 , B32B3/26 , B32B3/30 , B32B17/10036 , B32B17/10045 , B32B17/10119 , B32B17/10137 , C03B17/064 , C03B18/02 , C03B23/023 , C03C3/083 , C03C3/087 , C03C3/093 , C03C21/002 , B32B2315/08 , B32B2329/04 , B32B2329/06 , B32B2551/00 , B32B2571/00 , B32B2605/006 , Y10T428/24777
Abstract: A laminated glass pane is provided that includes a first glass sheet, a polymeric layer having a thickness between at least 0.5 mm and at most 1.7 mm, and a second inner glass sheet which has a thickness of at least 0.3 mm and at most 1.5 mm and is made of a lithium aluminum silicate glass. The polymeric layer is disposed between the at least two glass sheets. Furthermore, the glasses of the first and the second glass sheets are matched so that the temperatures at which the two glasses of the first and second glass sheets have the same viscosity in the viscosity range between 107 dPa·s and 1010 dPa·s differ from each other only by a maximum of 50° C.
-
公开(公告)号:US20210039981A1
公开(公告)日:2021-02-11
申请号:US16986191
申请日:2020-08-05
Applicant: SCHOTT AG
Inventor: Jochen Alkemper , Rüdiger Dietrich , Jovana Djordjevic-Reiss , Inge Burger
Abstract: A plate-shaped or disc-shaped, chemically prestressed or chemically prestressable glass article is provided. The article includes a glass with a composition of SiO2, Al2O3, and Li2O; and a set-drop strength of at least 50 and up to 150, given as drop height in cm, wherein the drop height is given as the mean value of 15 samples, with the use of a sandpaper grit of 60. The glass has one or more features including: a CIL of greater than 1 N, 1.2 N, 2N, or 3 N, a DoL of at least 90 μm, 100 μm, 115 μm, or 130 μm, a content of network formers of at least 82 wt. %, and a content of alkali oxides of at most 14 wt. % or 12 wt. %.
-
公开(公告)号:US09952378B2
公开(公告)日:2018-04-24
申请号:US15239191
申请日:2016-08-17
Applicant: SCHOTT AG
Inventor: Gerhard Lautenschläger , Thomas Kloss , Jochen Alkemper , Matthias Schmidt , Andreas Voitsch
CPC classification number: G02B6/0065 , C03C3/091 , C03C4/0092 , G02B6/0043
Abstract: A light guide plate for guiding of visible light for the backlighting of a liquid crystal display is provided. The light guide plate has two parallel lateral faces and at least one edge face, which serves preferably as a light input face. The light guide plate is a glass that contains B2O3 and SiO2 as components, wherein the total content of B2O3 and SiO2 is at least 70 weight percent and the B2O3 content is greater than 10%. The total content of metal oxide of divalent metals in the composition of the glass is less than 3 weight percent. Al2O3 is contained between 1 weight percent and 5 weight percent in the composition.
-
7.
公开(公告)号:US20230183128A1
公开(公告)日:2023-06-15
申请号:US18064873
申请日:2022-12-12
Applicant: SCHOTT AG , SCHOTT Technical Glass Solutions GmbH
Inventor: Ruediger Dietrich , Meike SCHNEIDER , Jochen Alkemper , Lars Mueller , Thomas Pfeiffer , Julian Koch , Bernd Ruedinger
CPC classification number: C03C21/002 , C03C10/0009 , C03C10/0054 , C03C2204/00
Abstract: A cover glass is provided that includes a silica based glass ceramic with a thickness between 0.4 mm and 0.85 mm. The glass ceramic has a transmittance of more than 80% from 380 nm to 780 nm and a stress attribute selected from: an overall compressive stress (CS) of at least 250 MPa and at most 1500 MPa, a compressive stress at a depth of 30 μm (CS30) from one of the two faces of at least 160 MPa and at most 525 MPa, a depth of the compression layer (DoCL) of at least 0.2 times the thickness and less than 0.5 times the thickness, and any combinations thereof. The glass ceramic has at least one silica based crystal phase having in a near-surface layer a unit cell volume of at least 1% by volume larger than that of a core where the crystal phase has minimum stresses.
-
公开(公告)号:US20200055769A1
公开(公告)日:2020-02-20
申请号:US16663788
申请日:2019-10-25
Applicant: SCHOTT AG
Inventor: Michael Schwall , Christian Mlx , Jochen Alkemper , Peter Thomas
Abstract: A thermally tempered glass element is provided made of glass with two opposite faces that are under compressive stress of at least 40 MPa. The glass has a working point at which the glass has a viscosity of 104 dPa·s of at most 1350° C. The glass has a viscosity versus temperature profile and a coefficient of thermal expansion versus temperature profile of the glass are such that a variable (750° C.−T13)/(CTELiq−CTESol) has a value of at most 5*106 K2. The CTELiq is a coefficient of linear thermal expansion of the glass above a glass transition temperature Tg, the CTESol is a coefficient of linear thermal expansion of the glass in a temperature range from 20° C. to 300° C., and the T13 is a temperature at which the glass has a viscosity of 1013 dPa·s.
-
公开(公告)号:US20170183255A1
公开(公告)日:2017-06-29
申请号:US15455759
申请日:2017-03-10
Applicant: Schott AG
Inventor: Marten Walther , Marta Krzyzak , Dirk Apitz , Jochen Alkemper
CPC classification number: C03C17/25 , C03B17/06 , C03C3/083 , C03C3/085 , C03C3/091 , C03C3/093 , C03C4/18 , C03C17/007 , C03C21/002 , C03C2204/00 , C03C2217/23 , C03C2217/76 , C03C2218/113 , C09D5/002
Abstract: A coated chemically strengthened flexible thin glass includes a coating of an adhesive layer in the form of a silicon mixed oxide layer, which contains or consists of a silicon oxide layer in combination with at least one oxide of aluminum, tin, magnesium, phosphorus, cerium, zirconium, titanium, cesium, barium, strontium, niobium, zinc, or boron, and magnesium fluoride, such as at least aluminum oxide.
-
公开(公告)号:US20170152171A1
公开(公告)日:2017-06-01
申请号:US15360370
申请日:2016-11-23
Applicant: SCHOTT AG
Inventor: Michael Schwall , Christian MIx , Jochen Alkemper , Peter Thomas
Abstract: A thermally tempered glass element is provided made of glass with two opposite faces that are under compressive stress of at least 40 MPa. The glass has a working point at which the glass has a viscosity of 104 dPa·s of at most 1350° C. The glass has a viscosity versus temperature profile and a coefficient of thermal expansion versus temperature profile of the glass are such that a variable (750° C.−T13)/(CTELiq−CTESol) has a value of at most 5*106 K2. The CTELiq is a coefficient of linear thermal expansion of the glass above a glass transition temperature Tg, the CTESol is a coefficient of linear thermal expansion of the glass in a temperature range from 20° C. to 300° C., and the T13 is a temperature at which the glass has a viscosity of 1013 dPa·s.
-
-
-
-
-
-
-
-
-