FERRITIC STAINLESS STEEL SHEET AND METHOD FOR MANUFACTURING THE SAME

    公开(公告)号:US20220170129A1

    公开(公告)日:2022-06-02

    申请号:US17442411

    申请日:2019-03-26

    Abstract: There is provided a ferritic stainless steel sheet having excellent corrosion resistance and excellent hydrogen embrittlement resistance without requiring dehydrogenation treatment during its manufacture or incorporating large amounts of Ni, Cu, or Mn.
    The ferritic stainless steel sheet has a chemical composition containing, by mass percent, C: 0.001% to 0.020%, Si: 0.10% to 0.60%, Mn: 0.10% to 0.60%, P: 0.040% or less, S: 0.030% or less, Al: 0.030% to 0.060%, Cr: 16.5% to 19.0%, Ti: 0.15% to 0.35% Nb: 0.30% to 0.60%, Ni: 0.01% to 0.60%, O (oxygen): 0.0025% to 0.0050%, and N: 0.001% to 0.020%, the balance being Fe and incidental impurities, in which the number of precipitates having a cross-sectional area of 5.0 μm2 or more is 300 or less in a 1-mm2 region, and the precipitates having a cross-sectional area of 5.0 μm2 or more has an average cross-sectional area of 20.0 μm2 or less.

    STAINLESS STEEL AND COPPER JOINED BODY, METHOD OF PRODUCING SAME, AND STAINLESS STEEL AND COPPER JOINING METHOD

    公开(公告)号:US20240367253A1

    公开(公告)日:2024-11-07

    申请号:US18688788

    申请日:2022-09-21

    Inventor: Shuji NISHIDA

    Abstract: A stainless steel and copper joined body is provided. A fillet welded lap joint that is a joined portion of stainless steel and copper is formed at an end of the copper. The Cu/Fe ratio of the fillet welded lap joint is 2.3 or more. The fillet welded lap joint includes multiple welding points that are continuous in the welding direction. The average diameter Dmean (mm) of the welding points and the copper thickness (mm) satisfy the relationship of the following Formula (1). The overlap ratio OR of welding points is 10% or more and 80% or less. 2 ⁢ t 0.5 ≤ D mean ≤ 10 ⁢ t 0.5 ( 1 )