Abstract:
A reed switch has a contact surface composed of three layers of metal applied to the contacts of the reed switch. The three layers comprise first a layer of titanium of approximately 15 to 150 micro inches, second a layer of molybdenum of 15 to 150 micro inches, and finally a contact layer of 5 to 20 micro inches of ruthenium, or other platinum group metal or alloy. The layers may be applied by any suitable methods, for example by sputtering.
Abstract:
A reed switch has a contact surface composed of three layers of metal applied to the contacts of the reed switch. The three layers comprise first a layer of titanium of approximately 15 to 150 micro inches, second a layer of molybdenum of 15 to 150 micro inches, and finally a contact layer of 5 to 20 micro inches of ruthenium, or other platinum group metal or alloy. The layers may be applied by any suitable methods, for example by sputtering.
Abstract:
In an encapsulated contact material which varies little in contact resistance and has good working life performance, at least one contact coating layer is formed covering the surface of a contact substrate. The contact coating layer includes a substantial matrix formed of at least one element selected from a group including Mo, Zr, Nb, Hf, Ta, and W, the matrix being loaded with 0.5 to 50 atom % of at least one element selected from a group including Zn, Cd, Hg, Al, Ga, In, Tl, Ge, Sn, Pb, As, Sb, and Bi. The contact coating layer has a thickness of 0.1 .mu.m or more.
Abstract:
Magnetically actuated devices such as, e.g., switches and synchronizers typically comprise a magnetically semihard component having a square B-H hysteresis loop and high remanent induction. Among alloys having such properties are Co-Fe-V, Co-Fe-Nb, and Co-Fe-Ni-Al-Ti alloys which, however, contain undesirably large amounts of cobalt.According to the invention, devices are equipped with a magnetically semihard, high-remanence Fe-Mo-Ni alloy which comprises Mo in a preferred amount in the range of 2-26 weight percent and Ni in a preferred amount in the range of 0.5-15 weight percent.Magnets made from alloys of the invention may be shaped, e.g., by cold drawing, rolling, bending, or flattening and may be used in devices such as, e.g., electrical contact switches, hysteresis motors, and other magnetically actuated devices.Preparation of alloys of the invention may be by a treatment of annealing and aging or deformation and aging.
Abstract:
A new type of electrical contact is described which has reduced erosion and sticking failures and has reduced material costs. The electrical contact is particularly suitable for sealed electrical contacts such as in sealed remreed contacts.