A NEW CROSSLINKED POLYMER COMPOSITION, STRUCTURED LAYER AND CABLE

    公开(公告)号:US20170233508A1

    公开(公告)日:2017-08-17

    申请号:US15504903

    申请日:2015-08-19

    申请人: BOREALIS AG

    摘要: The present invention relates to a crosslinked polymer composition comprising a crosslinked polyolefin, wherein the polymer composition comprises, prior to crosslinking, a polyolefin and peroxide which is in an amount of less than 35 mmol —O—O-/kg polymer composition, characterized in that the crosslinked polymer composition has been in a direct contact with a semiconductive composition for 24 h at 70° C., and that the crosslinked polymer composition thereafter has an electrical DC-conductivity of 150 fS/m or less, wherein the electrical DC-conductivity is measured in accordance with “DC conductivity method”, as described under “Determination methods”, on a plaque of the crosslinked polymer composition at 70° C. and 30 kV/mm mean electric field from a non-degassed and 1 mm thick plaque sample of the crosslinked polymer composition; a layered structure, cable, e.g. a power cable, use of the crosslinked polymer composition and the structured layer, both, for producing a crosslinked power cable, e.g., a cross linked direct current (DC) power cable; and a process for producing a cable.

    A NEW CROSSLINKED LOW MFR POLYMER COMPOSITION, POWER CABLE INSULATION AND POWER CABLE
    33.
    发明申请
    A NEW CROSSLINKED LOW MFR POLYMER COMPOSITION, POWER CABLE INSULATION AND POWER CABLE 审中-公开
    新型交联低MFR聚合物组合物,电力电缆绝缘和电力电缆

    公开(公告)号:US20160314869A1

    公开(公告)日:2016-10-27

    申请号:US15105230

    申请日:2014-08-19

    申请人: BOREALIS AG

    摘要: The present invention relates to a crosslinked polymer composition, which is obtained by crosslinking a polymer composition, which polymer composition has a melt flow rate (MFR) of less than 1.7 and comprises a polyolefm, peroxide and sulphur containing antioxidant, characterised by that the crosslinked polymer composition has an Oxidation Induction Time, determined according to ASTM-D3895, ISO/CD 11357 and EN 728 using a Differential Scanning Calorimeter (DSC), which Oxidation Induction Time corresponds to Z minutes, and comprises an amount of peroxide by-products which corresponds to W ppm determined according to BTM2222 using HPLC, wherein Z1≦Z≦Z2, W1≦W≦W2, and W≦p−270*Z, wherein Z1 is 0, Z2 is 60, W1 is 0 and W2 is 9500, and p is 18500; and use thereof, a power cable insulation and a power cable, useful in high voltage (HV) and extra high voltage (EHV) cable applications direct current (DC) applications.

    摘要翻译: 本发明涉及一种交联聚合物组合物,其通过交联聚合物组合物获得,该聚合物组合物的熔体流动速率(MFR)小于1.7,并且包含聚烯烃,过氧化物和含硫的抗氧化剂,其特征在于,交联的 聚合物组合物具有氧化诱导时间,其使用差示扫描量热计(DSC)根据ASTM-D3895,ISO / CD 11357和EN 728测定,氧化诱导时间对应于Z分钟,并且包含一定量的过氧化物副产物, 对应于根据BTM2222使用HPLC测定的W ppm,其中Z1≤Z≤Z2,W1≤W≤W2,W≤p-270×Z,其中Z1为0,Z2为60,W1为0,W2为9500, p为18500; 及其使用,电力电缆绝缘和电力电缆,可用于高压(HV)和超高压(EHV)电缆应用直流(DC)应用。