公开(公告)号:US11707863B2
公开(公告)日:2023-07-25
申请号:US17715579
申请日:2022-04-07
发明人: Mat T. Nielsen
CPC分类号: B28B19/0053 , B05D1/02 , B44F9/04
摘要: The present disclosure describes architectural blocks configured to give the appearance of real cut stone. A fresh plaster composition may be applied to one or more surfaces of a block, such as a concrete masonry unit (CMU) to form an architectural block having the appearance of cut stone. The fresh plaster composition includes a cementitious component, such as white Portland cement, water, a limestone aggregate component, and optionally an adhesive component. The limestone aggregate component includes a fine sand portion and a coarse sand portion that effectively enable the appearance of cut stone after finishing of the hardened or curted plaster surface via sanding and/or polishing.
-
公开(公告)号:US20210396005A1
公开(公告)日:2021-12-23
申请号:US17198642
申请日:2021-03-11
发明人: David L. Nicolson
摘要: The present disclosure describes modular blocks configured to give the appearance of natural or cut stone. An aesthetic coating composition may be applied to one or more surfaces of a block having a low-density, such as an insulating concrete form (ICF), to form an modular block having the appearance of cut stone. The aesthetic coating composition includes a binder component, such as a cementitious binder made from white Portland cement, or a polymer binder such as an acrylic binder, an aggregate component, such as a limestone aggregate component, and optionally an adhesive component. The aggregate component includes a fine sand portion and a coarse sand portion that effectively enable the appearance of cut stone after finishing of the aesthetic coating surface via sanding, polishing, sandblasting, acid etching, acid finishing, or exposed aggregate finishing.
-
13.
公开(公告)号:US09139473B2
公开(公告)日:2015-09-22
申请号:US14466604
申请日:2014-08-22
发明人: David L. Nicolson
CPC分类号: B01F3/1271 , B01F3/1214 , B01F15/0274 , B01F2215/0047 , B05B7/0433 , B05B7/0491 , B05B7/062 , B05D1/02 , C04B14/42 , C04B28/02 , C04B40/0028 , C04B2111/00129 , C04B2111/00155 , C04B24/2641 , C04B24/383 , C04B14/06 , C04B14/28 , C04B20/0096 , C04B2103/30 , C04B2103/34 , C04B2/02
摘要: Glass-fiber-reinforced concrete compositions that may be sprayed, and methods of preparing and applying such compositions. Such compositions may include cement, reinforcing glass fibers randomly oriented and homogenously distributed throughout the concrete composition, and a particle packing aggregate. At least a portion of the particle packing aggregate may be rounded rather than crushed and include a first aggregate portion having a first particle size and a second aggregate portion having a second particle size that is smaller than the first particle size so that the aggregate is capable of particle packing. The uncured compositions can be delivered through a spray nozzle with the glass fibers already mixed into the composition. The compositions can provide uniform, non-directional strength characteristics, e.g., modulus of rupture of at least 16 MPa and a limit of proportionality of at least 7 MPa with a glass-fiber content of no more than 4% by weight.
摘要翻译: 可以喷涂的玻璃纤维增强混凝土组合物,以及制备和施用这些组合物的方法。 这样的组合物可以包括水泥,随机取向并均匀地分布在整个混凝土组合物中的增强玻璃纤维和颗粒包装骨料。 颗粒填充聚集体的至少一部分可以是圆形的而不是破碎的,并且包括具有第一粒度的第一聚集体部分和具有小于第一粒度的第二粒度的第二聚集体部分,使得聚集体能够 的颗粒包装。 未固化的组合物可以通过已经混合到组合物中的玻璃纤维的喷嘴进行输送。 组合物可以提供均匀的非定向强度特性,例如至少16MPa的断裂模量和至少7MPa的玻璃纤维含量不超过4重量%的比例极限。
-
14.
公开(公告)号:US20140363580A1
公开(公告)日:2014-12-11
申请号:US14466604
申请日:2014-08-22
发明人: David L. Nicolson
CPC分类号: B01F3/1271 , B01F3/1214 , B01F15/0274 , B01F2215/0047 , B05B7/0433 , B05B7/0491 , B05B7/062 , B05D1/02 , C04B14/42 , C04B28/02 , C04B40/0028 , C04B2111/00129 , C04B2111/00155 , C04B24/2641 , C04B24/383 , C04B14/06 , C04B14/28 , C04B20/0096 , C04B2103/30 , C04B2103/34 , C04B2/02
摘要: Glass-fiber-reinforced concrete compositions that may be sprayed, and methods of preparing and applying such compositions. Such compositions may include cement, reinforcing glass fibers randomly oriented and homogenously distributed throughout the concrete composition, and a particle packing aggregate. At least a portion of the particle packing aggregate may be rounded rather than crushed and include a first aggregate portion having a first particle size and a second aggregate portion having a second particle size that is smaller than the first particle size so that the aggregate is capable of particle packing. The uncured compositions can be delivered through a spray nozzle with the glass fibers already mixed into the composition. The compositions can provide uniform, non-directional strength characteristics, e.g., modulus of rupture of at least 16 MPa and a limit of proportionality of at least 7 MPa with a glass-fiber content of no more than 4% by weight.
摘要翻译: 可以喷涂的玻璃纤维增强混凝土组合物,以及制备和施用这些组合物的方法。 这样的组合物可以包括水泥,随机取向并均匀地分布在整个混凝土组合物中的增强玻璃纤维和颗粒包装骨料。 颗粒填充聚集体的至少一部分可以是圆形的而不是破碎的,并且包括具有第一粒度的第一聚集体部分和具有小于第一粒度的第二粒度的第二聚集体部分,使得聚集体能够 的颗粒包装。 未固化的组合物可以通过已经混合到组合物中的玻璃纤维的喷嘴进行输送。 组合物可以提供均匀的非定向强度特性,例如至少16MPa的断裂模量和至少7MPa的玻璃纤维含量不超过4重量%的比例极限。
-
-
-