公开(公告)号:US20100196615A1
公开(公告)日:2010-08-05
申请号:US12755483
申请日:2010-04-07
申请人: Taiji TORIGOE , Ikuo OKADA , Tomoaki YUNOMURA , Hidetaka OGUMA , Toshio SAKON , Yutaka KAWATA
发明人: Taiji TORIGOE , Ikuo OKADA , Tomoaki YUNOMURA , Hidetaka OGUMA , Toshio SAKON , Yutaka KAWATA
CPC分类号: F02K9/974 , C23C4/073 , C23C10/02 , C23C10/08 , C23C10/26 , C23C28/321 , C23C28/3215 , C23C28/325 , C23C28/3455 , C23C30/00 , F01D5/288 , F05D2230/90 , F05D2260/95 , F05D2300/134 , F05D2300/15 , F05D2300/611 , Y10T428/12611 , Y10T428/12931 , Y10T428/12944
摘要: The present invention provides an oxidation-resistant coating having superior oxidation resistance and superior ductility and toughness for long-term use, and a method for forming the oxidation-resistant coating. An MCrAlY layer primarily containing an MCrAlY alloy (in which M indicates at least one element of Co and Ni) is formed on a substrate formed of a heat-resistant metal by thermal spraying or EB=PVD, and subsequently, aluminum is diffused into a part of the MCrAlY layer in the thickness direction thereof from a side opposite to the substrate.
摘要翻译: 本发明提供了具有优异的抗氧化性和长期使用的优异的延展性和韧性的耐氧化涂层以及形成抗氧化涂层的方法。 通过热喷涂或EB = PVD在由耐热金属形成的基板上形成主要含有MCrAlY合金(其中M表示Co和Ni的至少一种元素)的MCrAlY层,随后将铝扩散到 MCrAlY层的厚度方向的一部分与基板相反的一侧。