METHODS FOR ARTIFICIALLY AGING ALUMINUM-ZINC-MAGNESIUM ALLOYS, AND PRODUCTS BASED ON THE SAME
    1.
    发明申请
    METHODS FOR ARTIFICIALLY AGING ALUMINUM-ZINC-MAGNESIUM ALLOYS, AND PRODUCTS BASED ON THE SAME 有权
    用于人造铝镁合金的方法和基于其的产品

    公开(公告)号:US20150259774A1

    公开(公告)日:2015-09-17

    申请号:US14206448

    申请日:2014-03-12

    Applicant: ALCOA INC.

    CPC classification number: C22F1/053 C22C21/10 C22F1/002

    Abstract: New methods for aging aluminum alloys having zinc and magnesium are disclosed. The methods may include first aging the aluminum alloy at a first temperature of from about 310° F. to 530° F. and for a first aging time of from 1 minute to 6 hours, and then second aging the aluminum alloy at a second temperature for a second aging time of at least 30 minutes, with the second temperature being lower than the first temperature.

    Abstract translation: 公开了具有锌和镁的老化铝合金的新方法。 所述方法可以包括在约310°F至530°F的第一温度和1分钟至6小时的第一老化时间之前对铝合金进行老化,然后在第二温度下对铝合金进行二次老化 第二老化时间至少为30分钟,第二温度低于第一温度。

    METHODS FOR ARTIFICIALLY AGING ALUMINUM-ZINC-MAGNESIUM ALLOYS, AND PRODUCTS BASED ON THE SAME
    2.
    发明申请
    METHODS FOR ARTIFICIALLY AGING ALUMINUM-ZINC-MAGNESIUM ALLOYS, AND PRODUCTS BASED ON THE SAME 有权
    用于人造铝镁合金的方法和基于其的产品

    公开(公告)号:US20150376754A1

    公开(公告)日:2015-12-31

    申请号:US13827918

    申请日:2013-03-14

    Applicant: ALCOA INC.

    CPC classification number: C22F1/053 C22C21/10

    Abstract: New methods for aging aluminum alloys having zinc and magnesium are disclosed. The methods may include first aging the aluminum alloy at a first temperature of from about 330° F. to 530° F. and for a first aging time of from 1 minute to 6 hours, and then second aging the aluminum alloy at a second temperature for a second aging time of at least 30 minutes, with the second temperature being lower than the first temperature.

    Abstract translation: 公开了具有锌和镁的老化铝合金的新方法。 所述方法可以包括在约330°F至530°F的第一温度和1分钟至6小时的第一老化时间之前首先老化铝合金,然后在第二温度下对铝合金进行二次老化 第二老化时间至少为30分钟,第二温度低于第一温度。

    Methods for artificially aging aluminum-zinc-magnesium alloys, and products based on the same
    3.
    发明授权
    Methods for artificially aging aluminum-zinc-magnesium alloys, and products based on the same 有权
    人造老化铝锌镁合金的方法及其制品

    公开(公告)号:US09249487B2

    公开(公告)日:2016-02-02

    申请号:US13827918

    申请日:2013-03-14

    Applicant: Alcoa Inc.

    CPC classification number: C22F1/053 C22C21/10

    Abstract: New methods for aging aluminum alloys having zinc and magnesium are disclosed. The methods may include first aging the aluminum alloy at a first temperature of from about 330° F. to 530° F. and for a first aging time of from 1 minute to 6 hours, and then second aging the aluminum alloy at a second temperature for a second aging time of at least 30 minutes, with the second temperature being lower than the first temperature.

    Abstract translation: 公开了具有锌和镁的老化铝合金的新方法。 所述方法可以包括在约330°F至530°F的第一温度和1分钟至6小时的第一老化时间之前首先老化铝合金,然后在第二温度下对铝合金进行二次老化 第二老化时间至少为30分钟,第二温度低于第一温度。

Patent Agency Ranking