Invention Grant
US09452578B2 Fast firing method for high porosity ceramics 有权
高孔隙陶瓷的快速烧制方法

Fast firing method for high porosity ceramics
Abstract:
A method for firing a green honeycomb ceramic body including heating the green honeycomb ceramic body from room temperature to a first temperature of less than or equal to about 350° C. with at least one heating rate of greater than or equal to about 80° C./hr. The green honeycomb ceramic body may be heated from the first temperature to a second temperature of greater than or equal to about 800° C. at a heating rate of greater than or equal to about 90° C./hr. The green honeycomb ceramic body may be heated from the second temperature to a third temperature of greater than or equal to about 1000° C. The green honeycomb ceramic body may include aluminum raw materials for forming an aluminum titanate ceramic body.