发明授权
US08721948B2 Process for producing crosslinked fluororubber 有权
制备交联氟橡胶的方法

  • 专利标题: Process for producing crosslinked fluororubber
  • 专利标题(中): 制备交联氟橡胶的方法
  • 申请号: US12160427
    申请日: 2006-10-16
  • 公开(公告)号: US08721948B2
    公开(公告)日: 2014-05-13
  • 发明人: Hiroyuki SanoHiroki Matsumoto
  • 申请人: Hiroyuki SanoHiroki Matsumoto
  • 申请人地址: JP Tokyo
  • 专利权人: NOK Corporation
  • 当前专利权人: NOK Corporation
  • 当前专利权人地址: JP Tokyo
  • 代理机构: Crockett & Crockett, PC
  • 代理商 K. David Crockett, Esq.; Niky Economy Syrengelas, Esq.
  • 优先权: JP2006-004269 20060111
  • 国际申请: PCT/JP2006/320585 WO 20061016
  • 国际公布: WO2007/080681 WO 20070719
  • 主分类号: B29C71/02
  • IPC分类号: B29C71/02
Process for producing crosslinked fluororubber
摘要:
[Problem]To provide a method for producing a polyol-crosslinking, crosslinked fluororubber product which exhibits low tack properties and significantly increased rubber hardness.[Means for Solving the problem] The method comprises pressurizing, heating, and vulcanizing a fluororubber composition to mold a vulcanized product; the fluororubber composition comprising a polyol-crosslinkable fluororubber, a crosslinking accelerator including a quarternary phosphonium salt or a quarternary ammonium salt, and a polyol crosslinking agent, the weight ratio X of the crosslinking accelerator to the polyol crosslinking agent (crosslinking accelerator/polyol crosslinking agent) being from 0.90 to 3.00 for a quarternary phosphonium salt, and being from 0.4 to 0.6 for a quarternary ammonium salt; applying a treatment solution containing the polyol crosslinking agent and the crosslinking accelerator dissohttp://reedman/Manuals/Text_Manual/Section_03.htm - 3.1lved in a solvent to a surface of the vulcanized product; and heat-treating the resulting vulcanized product at a temperature ranging from 200 to 300° C. for 1 to 20 hours.