Invention Application
US20120064344A1 METHOD FOR PRODUCING ALKALI METAL NIOBATE PARTICLES, AND ALKALI METAL NIOBATE PARTICLES
有权
生产碱性金属非离子表面活性剂的方法,以及碱金属氨基化物
- Patent Title: METHOD FOR PRODUCING ALKALI METAL NIOBATE PARTICLES, AND ALKALI METAL NIOBATE PARTICLES
- Patent Title (中): 生产碱性金属非离子表面活性剂的方法,以及碱金属氨基化物
-
Application No.: US13262770Application Date: 2010-04-05
-
Publication No.: US20120064344A1Publication Date: 2012-03-15
- Inventor: Atsushi Muramatsu , Kiyoshi Kanie , Atsuki Terabe , Yasuhiro Okamoto , Hideto Mizutani , Satoru Sueda , Hirofumi Takahashi
- Applicant: Atsushi Muramatsu , Kiyoshi Kanie , Atsuki Terabe , Yasuhiro Okamoto , Hideto Mizutani , Satoru Sueda , Hirofumi Takahashi
- Applicant Address: JP Sakai-shi, Osaka JP Fujinomiya-shi, Shizuoka JP Sendai-shi, Miyagi
- Assignee: SAKAI CHEMICAL INDUSTRY CO., LTD.,FUJI CERAMICS CORPORATION,TOHOKU UNIVERSITY
- Current Assignee: SAKAI CHEMICAL INDUSTRY CO., LTD.,FUJI CERAMICS CORPORATION,TOHOKU UNIVERSITY
- Current Assignee Address: JP Sakai-shi, Osaka JP Fujinomiya-shi, Shizuoka JP Sendai-shi, Miyagi
- Priority: JP2009-095013 20090409
- International Application: PCT/JP2010/056171 WO 20100405
- Main IPC: C01G33/00
- IPC: C01G33/00

Abstract:
Disclosed are a method of producing fine particulate alkali metal niobate in a liquid phase system, wherein the size and shape of the particulate alkali metal niobate can be controlled; and fine particulate alkali metal niobate having a controlled shape and size. One of specifically disclosed is a method of producing a substantially rectangular cuboid particulate alkali metal niobate represented by MNbO3 (1), wherein M represents one element selected from alkaline metals, including specific four steps. Another one of specifically disclosed is particulate alkali metal niobate represented by the formula (1) having a substantially rectangular cuboid shape, wherein the substantially rectangular cuboid shape has a longest side and a shortest side, the length of the longest side represented by an index Lmax is 0.10 to 25 μm, and the length of the shortest side represented by an index Lmin is 0.050 to 15 μm.
Public/Granted literature
- US08771618B2 Method for producing alkali metal niobate particles, and alkali metal niobate particles Public/Granted day:2014-07-08