- 专利标题: High-strength martensite heat resisting cast steel, method of producing the steel, and applications of the steel
- 专利标题(中): 高强度马氏体耐热铸钢,钢的生产方法和钢的应用
-
申请号: US11528474申请日: 2006-09-28
-
公开(公告)号: US20100122754A1公开(公告)日: 2010-05-20
- 发明人: Hirotsugu Kawanaka , Masahiko Arai , Hideo Yoda
- 申请人: Hirotsugu Kawanaka , Masahiko Arai , Hideo Yoda
- 优先权: JP2005-283198 20050929
- 主分类号: C21D8/00
- IPC分类号: C21D8/00 ; C22C38/44 ; C22C38/46 ; C22C38/48 ; C22C38/52 ; C22C38/54
摘要:
A high-strength martensite heat resisting steel which has long-time creep rupture strength required for steam temperature condition of 600-630° C. and toughness at room temperature, and which is suitable for use as a material of a steam turbine rotor shaft and as large-sized forged steel with an improvement of hot forgeability. A method of producing the steel and applications of the steel are also provided. The high-strength martensite heat resisting steel contains 0.05-0.20% by mass of C, 0.1% or less of Si, 0.05-0.6% of Mn, 0.1-0.6% of Ni, 9.0-12.0% of Cr, 0.20-0.65% of Mo, 2.0-3.0% of W, 0.1-0.3% of V, 2.0% or less of Co, 0.02-0.20% of Nb, 0.015% or less of B, 0.01-0.10% of N, and 0.015% or less of Al, (W/Mo) being 4.0-10.0.
信息查询