Method for modification of surface of optical fiber preform
Abstract:
The present disclosure provides a method for modification of surface of an initial optical fiber preform. The initial optical fiber preform is manufactured using at least one preform manufacturing process. The surface of the initial optical fiber preform is treated with 50-70 liters of chlorine per square meter of the surface of the initial optical fiber preform. The surface of the initial optical fiber preform is flame polished using a flame polishing module. The treatment of the surface of the initial optical fiber preform with chlorine and flame polishing of the surface of the initial optical fiber preform collectively converts the initial optical fiber preform into a modified optical fiber preform.
Public/Granted literature
Information query
Patent Agency Ranking