A graphene foam ceramic composite (GrF-CC) comprises an open cell graphene foam (GrF) surrounded by and infiltrated with a sintered low temperature co-fired ceramic (LTCC) matrix. The GrF-CC can be prepared by infiltrating an open cell GrF with an LTCC slurry, removing the solvent from the slurry with solidification to a ceramic-GrF green body, and sintering the ceramic-GrF green body to form the GrF-CC. Sintering by spark plasma sintering (SPS) allows an LTCC GrF-CC that has a density of at least 90%.